NTIS 바로가기Corrosion science and technology, v.7 no.2, 2008년, pp.112 - 118
Morimoto, J. (Graduate School of Engineering, University of Hyogo) , Yamashita, M. (Graduate School of Engineering, University of Hyogo) , Uchida, H. (Graduate School of Engineering, University of Hyogo) , Doi, T. (Corporate Research and Development Laboratories Sumitomo Metal Industries, Ltd.) , Kamimura, T. (Corporate Research and Development Laboratories Sumitomo Metal Industries, Ltd) , Miyuki, H. (Corporate Research and Development Laboratories Sumitomo Metal Industries, Ltd.) , Konishi, H. (Synchrotron Radiation Research Center, Japan Atomic Energy Agency) , Mizuki, J. (Synchrotron Radiation Research Center, Japan Atomic Energy Agency)
We observed initial rusting process of steel containing Al under wet/dry cyclic condition with NaCl solution film using in situ X-ray diffraction spectroscopy at SPring-8 synchrotron radiation facility. It was found that mass fraction of iron oxides such as
* AI 자동 식별 결과로 적합하지 않은 문장이 있을 수 있으니, 이용에 유의하시기 바랍니다.
N. Wagure, K. Kashima, T. Kamimura and H. Miyuki, Proceedings of the 51st Japan Conference on Materials and Environments, p.175 (2004)
M. Yamashita, H. Konishi, T. Kozakura, J. Mizuki, and H. Uchida, Corrosion Science, 47, 2492 (2005)
S. Hara, M. Yamashita, T. Kamimura, M. Sato, J. Japan Inst. Metals, (2007) in press
T. Kamimura, N. Wagure, K. Kashima, T. Doi, H. Miyuki, S. Nasu and S. Morimoto, CAMP-ISIJ, 18, 1675 (2005)
※ AI-Helper는 부적절한 답변을 할 수 있습니다.