Nah, Hwan-Seon (Structural Engineering Lab., Korea Electric Power Research Institute) , Kim, Kang-Seok (Structural Engineering Lab., Korea Electric Power Research Institute) , Kim, Kang-Sik (Structural Engineering Lab., Korea Electric Power Research Institute) , Lee, Chul-Woo (Korea Power Engineering Co. Inc.) , Baker, Randy (S. G. Pinney Inc.)
An evaluation of underwater - repair coating materials was based on the premise that defective areas of the existent epoxy coating such as blistering and cracking will be repaired on spot under submerged condition. Tests include the clarification as to whether they are compatible between as-built co...
* AI 자동 식별 결과로 적합하지 않은 문장이 있을 수 있으니, 이용에 유의하시기 바랍니다.
Canadian Standard Association, Material Requirements for Concrete Containment Structure for CANDU Nuclear Power Plants, CAN3-N287.2-M82 (1982)
H.S. Nah and K.J. Kwon, Maintenance of Integrity for Non-metallic Liner Coated on Spent Fuel Bay, Research Report, July (2003)
H.S. Nah and K.J. Kwon, Feasibility Study on Investigation of Additional Repairing Methods for Non-Metallic Liner of Spent Fuel Bay, Research Report, Oct. (2006)
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.