A stainless steel having excellent pitting corrosion resistance and hot workability which comprises 0.001 to 0.20% (by weight) of C, 0.1 to 6.0% of Si, 0.1 to 10.0% of Mn, 15 to 35% of Cr, 3.5 to 35.0% of Ni, 0.01 to 6.0% of Mo (Si+Cr+Ni+Mo≥25%), 0.001 to 0.50% of N, 0.01 to 0.07% of Al, and 0.001 t
A stainless steel having excellent pitting corrosion resistance and hot workability which comprises 0.001 to 0.20% (by weight) of C, 0.1 to 6.0% of Si, 0.1 to 10.0% of Mn, 15 to 35% of Cr, 3.5 to 35.0% of Ni, 0.01 to 6.0% of Mo (Si+Cr+Ni+Mo≥25%), 0.001 to 0.50% of N, 0.01 to 0.07% of Al, and 0.001 to 0.02% of Ca with the balance being iron and unavoidable impurities.
대표청구항▼
A stainless steel having excellent pitting corrosion resistance and hot workability consisting of 0.001 to 0.20% (by weight) of C, 0.1 to 6.0% of Si, 0.1 to 10.0% of Mn, 17 to 27% of Cr, 10.0 to 20.0% of Ni, 0.01 to 6.0% of Mo (Si+Cr+Ni+Mo≥25%), 0.001 to 0.50% of N, 0.01 to 0.07% of Al, and 0.001 to
A stainless steel having excellent pitting corrosion resistance and hot workability consisting of 0.001 to 0.20% (by weight) of C, 0.1 to 6.0% of Si, 0.1 to 10.0% of Mn, 17 to 27% of Cr, 10.0 to 20.0% of Ni, 0.01 to 6.0% of Mo (Si+Cr+Ni+Mo≥25%), 0.001 to 0.50% of N, 0.01 to 0.07% of Al, and 0.001 to 0.02% of Ca with the balance being iron and unavoidable impurities.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.