Damage in a blisk airfoil is machined away to create a notch. A repair is welded in the airfoil to fill the notch. The weld repair is then machined to restore the airfoil to a substantially original, pre-damaged configuration at the repair.
대표청구항
▼
Damage in a blisk airfoil is machined away to create a notch. A repair is welded in the airfoil to fill the notch. The weld repair is then machined to restore the airfoil to a substantially original, pre-damaged configuration at the repair. 90 percent by volume of the oil phase and about 10 to abou
Damage in a blisk airfoil is machined away to create a notch. A repair is welded in the airfoil to fill the notch. The weld repair is then machined to restore the airfoil to a substantially original, pre-damaged configuration at the repair. 90 percent by volume of the oil phase and about 10 to about 80 percent of the aqueous phase, wherein the asphaltenes precipitate out of the emulsion and the emulsion demulsifies; and separating the aqueous phase from the oil phase such that the crude oil is recovered. 13. The method according to claim 12, wherein the carbon dioxide containing fluid contains a co-solvent. 14. The method according to claim 13, wherein the co-solvent is selected from the group consisting of methane, ethane, propane, ammonium-butane, n-pentane, hexanes, cyclohexane, n-heptane, methanol, ethanol, isopropanol, ethylene glycol, propylene glycol, methyl-isopropyl ketone, benzene, toluene, xylenes, terpenes, paraffins, and mixtures thereof. 15. The method according to claim 13, wherein the co-solvent is selected from the group consisting of n-heptane, toluene, and mixtures thereof. 16. The method according to claim 12, wherein the crude oil is a light crude oil. 17. The method according to claim 12, wherein the crude oil is a heavy crude oil. 18. The method according to claim 12, wherein said step of contacting the carbon dioxide containing fluid with the emulsion is carried out from about 30 minutes to about 24 hours. 19. The method according to claim 12, wherein the asphaltenes are present in an amount ranging from about 0.2 to about 25 percent (w/w). 20. The method according to claim 12, wherein the aqueous phase comprises at least one inorganic salt. 21. The method according to claim 20, wherein the inorganic salt is selected from the group consisting of sodium chloride, calcium chloride, magnesium chloride, sodium carbonate, magnesium sulfate, and mixtures thereof. 22. The method according to claim 12, wherein the inorganic salt has a concentration in the aqueous phase ranging from above about 0 to about 10 weight/volume percent. 23. A method of demulsifying a water-in-oil emulsion comprising an oil phase and an aqueous phase, the oil phase comprising crude oil including asphaltenes, said method comprising: adding the emulsion into a pressurizable vessel; contacting the emulsion with carbon dioxide containing fluid, wherein the pressure of the carbon dioxide containing fluid ranges from about 1000 psi to about 4500 psi, and the temperature of the carbon dioxide fluid ranges from about 25° C. to about 70° C., such that the carbon dioxide containing fluid enters the oil phase of the emulsion, the emulsion comprising from about 20 to about 90 percent by volume of the oil phase and about 10 to about 80 percent of the aqueous phase, wherein the asphaltenes precipitate out of the emulsion and the emulsion demulsifies; and separating the aqueous phase from the oil phase such that the crude oil is recovered. 24. The method according to claim 23, wherein the temperature of the carbon dioxide fluid ranges from 50° C. to about 70° C. 25. The method according to claim 23, wherein the temperature of the carbon dioxide fluid ranges from about 60° C. to about 70° C. 26. The method according to claim 23, wherein the pressure of the carbon dioxide fluid ranges from about 3000 psi to about 4500 psi. 27. The method according to claim 23, wherein the carbon dioxide containing fluid comprises supercritical carbon dioxide. 28. The method according to claim 23, wherein the carbon dioxide containing fluid contains a co-solvent. 29. The method according to claim 28, wherein the co-solvent is selected from the group consisting of n-pentane, hexanes, cyclohexane, n-heptane, methanol, ethanol, isopropanol, ethylene glycol, propylene glycol, methyl-isopropyl ketone, benzene, toluene, xylenes, terpenes, paraffins, and mixtures thereof. 30. The method according to claim 28, wherein the co-solvent is selected from the group consisting of n-heptane, toluene, and mixtures thereof. 31. The method according to claim 23, wherein the crude oil is a light crude oil. 32. The method according to claim 23, wherein the crude oil is a heavy crude oil. 33. The method accordi