초록
▼
Disclosed is fiber-reinforced thermoplastic resin pellets that satisfy the quality stability (homogeneous impregnation, deterioration prevention of reinforcing fiber) of the molding material and the strength performance of the molded product, using natural discontinuous fiber as the reinforcing fibe
Disclosed is fiber-reinforced thermoplastic resin pellets that satisfy the quality stability (homogeneous impregnation, deterioration prevention of reinforcing fiber) of the molding material and the strength performance of the molded product, using natural discontinuous fiber as the reinforcing fiber, and a manufacturing method of the pellets. A plurality of spun yarns with No. 5 to 80 counts are twisted 10 to 200 turns/m and pultruded when fiber-reinforced thermoplastic pellets containing natural fiber as the reinforcing fiber are manufactured by the impregnating pultrusion method.
대표청구항
▼
1. Natural fiber-reinforced thermoplastic resin pellets comprising thermoplastic resin and a strand comprising a plurality of spun yarns of natural fiber twisted in a range from 10 to 200 turns/m, wherein the spun yarns are No. 5 to 80 counts in diameter. 2. A method for manufacturing natural f
1. Natural fiber-reinforced thermoplastic resin pellets comprising thermoplastic resin and a strand comprising a plurality of spun yarns of natural fiber twisted in a range from 10 to 200 turns/m, wherein the spun yarns are No. 5 to 80 counts in diameter. 2. A method for manufacturing natural fiber-reinforced thermoplastic resin pellets comprising steps of: an impregnating step for impregnating in a thermoplastic resin bath, a plurality of spun yarns of natural fiber being No. 5 to 80 counts in diameter, a pultruding step for pultruding the spun yarns with twisting 10 to 200 turns/m to obtain natural fiber-reinforced thermoplastic resin, and a pelletizing step for pelletizing the natural fiber-reinforced thermoplastic resin. 3. A natural fiber-reinforced thermoplastic resin-made automobile part prepared from a composite comprising natural fiber-reinforced thermoplastic resin pellets comprising thermoplastic resin and a strand comprising a plurality of spun yarns of natural fiber twisted in a range from 10 to 200 turns/m, wherein the spun yarns are No. 5 to 80 counts in diameter. 4. The pellets according to claim 1, wherein the fiber is at least one selected from the group consisting of flax, ramie, abaca, sisal, jute, hemp, kenaf, Boehimeria nipponivea fiber, Japanese ramie, coir, cotton, kapok, hemp palm, rice straw, wheat straw, pineapple fiber, wool, and silk. 5. The pellets according to claim 1, wherein the spun yarns are No. 7 to 80 count. 6. The pellets according to claim 5, wherein the spun yarns are No. 10 to 40 count. 7. The pellets according to claim 1, wherein the plurality of spun yarns are twisted in a range of from 15 to 150 turns/m. 8. The pellets according to claim 7, wherein the plurality of spun yarns are twisted in a range of from 20 to 120 turns/m. 9. The pellets according to claim 1, wherein Z-twisting is employed for the spun yarns of natural fiber. 10. The pellets according to claim 9, wherein the spun yarns are No. 5 to 20 counts in diameter. 11. The pellets according to claim 1, wherein S-twisting is employed for the spun yarns of natural fiber. 12. The pellets according to claim 11, wherein the spun yarns are No. 21 to 80 counts in diameter. 13. The pellets according to claim 1, wherein the thermoplastic resin is at least one selected from the group consisting of polyolefin resins, polyamide resins, polyester resins, polycarbonate resins, polystyrene resins, acrylic resins, AS resins, ABS resins, PPS resins and POM resins. 14. The pellets according to claim 13, wherein the thermoplastic resin is at least one selected from the group consisting of polypropylene, high density polyethylene, linear low density polyethylene, low density polyethylene, polymers and copolymers of α-olefins, polyolefin resins modified with an unsaturated carboxylic acid or derivatives thereof, and ethylene-vinyl acetate resins. 15. The pellets according to claim 1, wherein the pellet has a length of 2 to 24 mm and a diameter of 1 to 5 mm. 16. The pellets according to claim 15, wherein the pellet length is 3 to 15 mm and the pellet diameter is 2 to 4 mm. 17. The pellets according to claim 1, wherein the aspect ratio of pellet length to pellet diameter ranges from 1 to 6. 18. The pellets according to claim 17, wherein the aspect ratio of pellet length to pellet diameter ranges from 2 to 5. 19. The pellets according to claim 1, wherein the natural fiber content is 10 to 65% by volume. 20. The pellets according to claim 19, wherein the natural fiber content is 12 to 60% by volume. 21. The pellets according to claim 1, wherein the natural fiber is discontinuous. 22. The pellets according to claim 1, wherein said plurality of spun yarns has a fixed length longer than a length of the pellet.