A directionally solidified nickel-base superalloy article has a defect therein extending parallel to the solidification direction. The article is repaired by removing any foreign matter present in the defect, and then heating the article to a repair temperature of from about 60 to about 98 percent o
A directionally solidified nickel-base superalloy article has a defect therein extending parallel to the solidification direction. The article is repaired by removing any foreign matter present in the defect, and then heating the article to a repair temperature of from about 60 to about 98 percent of the solidus temperature of the base material in a chamber containing a protective gas that inhibits oxidation of the base material. The defect is filled with a filler metal while maintaining the article at the repair temperature. The filling is accomplished by providing a source of the filler metal of substantially the same composition as the base material of the directionally solidified article, and melting the filler metal into the defect progressively while moving the source of the filler metal relative to the article in a direction parallel to the solidification direction. Optionally, additional artificial heat extraction is accomplished in a heat-flow direction that is within about 45 degrees of the solidification direction, as the filler metal solidifies within the defect. The article may thereafter be heat treated.
대표청구항▼
A directionally solidified nickel-base superalloy article has a defect therein extending parallel to the solidification direction. The article is repaired by removing any foreign matter present in the defect, and then heating the article to a repair temperature of from about 60 to about 98 percent o
A directionally solidified nickel-base superalloy article has a defect therein extending parallel to the solidification direction. The article is repaired by removing any foreign matter present in the defect, and then heating the article to a repair temperature of from about 60 to about 98 percent of the solidus temperature of the base material in a chamber containing a protective gas that inhibits oxidation of the base material. The defect is filled with a filler metal while maintaining the article at the repair temperature. The filling is accomplished by providing a source of the filler metal of substantially the same composition as the base material of the directionally solidified article, and melting the filler metal into the defect progressively while moving the source of the filler metal relative to the article in a direction parallel to the solidification direction. Optionally, additional artificial heat extraction is accomplished in a heat-flow direction that is within about 45 degrees of the solidification direction, as the filler metal solidifies within the defect. The article may thereafter be heat treated. -3692224, 19720900, Astafiev et al.; US-3774615, 19731100, Lim et al.; US-3805793, 19740400, Wright; US-3915399, 19751000, Kron et al.; US-4009841, 19770300, Matalia, 003/077; US-4076162, 19780200, Kapitanov et al.; US-4166466, 19790900, Jarvik, 009/079; US-4304236, 19811200, Conta et al.; US-4319576, 19820300, Rothfuss; US-4325376, 19820400, Klieman et al.; US-4350160, 19820900, Kolesov et al.; US-4352358, 19821000, Angelchik; US-4366819, 19830100, Kaster; US-4368736, 19830100, Kaster; US-4466436, 19840800, Lee; US-4505414, 19850300, Filipi; US-4523592, 19850600, Daniel; US-4553542, 19851100, Schenck et al.; US-4573468, 19860300, Conta et al.; US-4576167, 19860300, Noiles; US-4586503, 19860500, Kirsch et al.; US-4592354, 19860600, Rothfuss; US-4593693, 19860600, Schenck; US-4603693, 19860800, Conta et al.; US-4607637, 19860800, Berggren et al.; US-4624255, 19861100, Schenck et al.; US-4624257, 19861100, Berggren et al.; US-4646745, 19870300, Noiles; US-4657019, 19870400, Walsh et al.; US-4665906, 19870500, Jervis; US-4700703, 19871000, Resnick et al.; US-4703887, 19871100, Clanton et al.; US-4747407, 19880500, Liu et al.; US-4763851, 19880800, Flament; US-4907591, 19900300, Vasconcellos et al.; US-4917087, 19900400, Walsh et al.; US-4917090, 19900400, Berggren et al.; US-4917091, 19900400, Berggren et al.; US-4936942, 19900600, Sollinger et al.; US-4957499, 19900900, Lipatov et al.; US-5119983, 19920600, Green et al.; US-5197649, 19930300, Bessler et al.; US-5234447, 19930800, Kaster et al.; US-5242457, 19930900, Akopov; US-5271543, 19931200, Grant et al.; US-5292053, 19940300, Bilotti et al.; US-5324447, 19940600, Lam et al.; US-5330503, 19940700, Yoon; US-5333773, 19940800, Main et al.; US-5336233, 19940800, Chen; US-5348259, 19940900, Blanco et al.; US-5366462, 19941100, Kastger et al.; US-5395030, 19950300, Kuramoto et al.; US-5403333, 19950400, Kaster et al.; US-5478354, 19951200, Tovey et al.; US-5522834, 19960600, Fonger et al.; US-5549619, 19960800, Peters et al.; US-5554162, 19960900, DeLange; US-5620452, 19970400, Yoon; US-5669918, 19970900, Balazs et al.; US-5855312, 19990100, Toledano; US-5868760, 19990200, McGuckin, Jr.; US-5881943, 19990300, Heck et al.; US-5947363, 19990900, Bolduc et al.; US-6040748, 20000300, Gueissaz; US-6176413, 20010100, Heck et al., 227/179.1; US-6209773, 20010400, Bolduc et al., 606/219; US-6253984, 20010700, Heck et al., 227/175.1; US-6450390, 20020900, Heck et al., 227/019
연구과제 타임라인
LOADING...
LOADING...
LOADING...
LOADING...
LOADING...
이 특허에 인용된 특허 (14)
Dzugan Robert (Cincinnati OH) Ferrigno Stephen J. (Cincinnati OH) Young William R. (Cincinnati OH) Froning Marc J. (Tolland CT), Fabrication of cast articles from high melting temperature superalloy compositions.
Smashey Russell W. ; Snyder John H. ; Boerger Eric J. ; Borne Bruce L., Method for welding an article and terminating the weldment within the perimeter of the article.
Saltzman Gilbert A. (Howell NJ) Wertz Timothy A. (Manahawkin NJ) Friedman Ira L. (Rumson NJ), Method of refurbishing cast gas turbine engine components and refurbished component.
Clark Jeffrey J. (Tempe AZ) Fisk Harry R. (Tempe AZ) Wallace Larry A. (Tempe AZ), Weldable nickel base cast alloy for high temperature applications and method.
Hunt, Mark L.; Dimascio, Paul Stephen; Miglietti, Warren Martin; Byam, Steve P.; O'Connell, Matthew James, Composite turbine blade and method of manufacture.
Smith, Alistair Jeffrey; Demo, Wayne Alan; Galley, Ronald Lance; Italiano, Anthony Philip, Method, system, and computer software code for repairing a transition section of an engine.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.