A process for producing fine particulate polymer drag reducing agent (DRA) without cryogenic temperatures, is described. The grinding or pulverizing of polymer, such as poly(alpha-olefin) may be achieved by the use of at least one solid organic grinding aid and at least one liquid grinding aid. In o
A process for producing fine particulate polymer drag reducing agent (DRA) without cryogenic temperatures, is described. The grinding or pulverizing of polymer, such as poly(alpha-olefin) may be achieved by the use of at least one solid organic grinding aid and at least one liquid grinding aid. In one non-limiting embodiment of the invention, the grinding is conducted at ambient temperature. Examples of a solid organic grinding aid include ethene/butene copolymer particles, paraffin waxes and solid alcohols. An example of a suitable liquid grinding aid includes a blend of glycol, water and isopropyl alcohol. Particulate DRA may be produced at a size of about 500 microns or less. Use of an attrition mill is preferred.
대표청구항
▼
1. A method for producing a particulate polymer drag reducing agent, comprising:feeding to a mill components comprising: granulated polymer; at least one solid organic grinding aid; and a liquid grinding aid; and grinding the components to produce particulate polymer drag reducing agent. 2. The meth
1. A method for producing a particulate polymer drag reducing agent, comprising:feeding to a mill components comprising: granulated polymer; at least one solid organic grinding aid; and a liquid grinding aid; and grinding the components to produce particulate polymer drag reducing agent. 2. The method of claim 1 where in the feeding, the granulated polymer has a size between about 8 mm and about 12 mm.3. The method of claim 1 where in the feeding, the granulated polymer is poly(alpha-olefln).4. The method of claim 1 where in the feeding, the solid organic grinding aid has a size between about 1 and about 50 microns.5. The method of claim 1 where in the feeding, the solid organic grinding aid is selected from the group consisting of ethene/butene copolymer, paraffin waxes, solid alcohols, and mixtures thereof.6. The method of claim 1 where in the feeding, the liquid grinding aid is a blend of at least one glycol selected from the group consisting of ethylene glycol, propylene glycol, diethylene glycol, dipropylene glycol, methyl ethers of such glycols, and mixtures thereof, and at least one other liquid selected from the group consisting of water and at least one alcohol, the alcohol being selected from the group consisting of methanol, ethanol, isopropanol and mixtures thereof.7. The method of claim 1 where in the feeding, the liquid grinding aid is a blend of ethylene glycol, water and isopropanol where the proportions range from about 20 to 80 wt. % to about 20 to 80 wt. % to about 0 to 30 wt. %.8. The method of claim 1 where in the feeding, the granulated polymer is fed at a rate of from about 100 to about 300 lbs/hr (45-138 kg/hr) the solid organic grinding aid is fed at a rate of from about 10 to about 90 lbs/hr (4.5-41 kg/hr) and the liquid grinding aid is fed at a rate of from about 0.01 to about 0.5 gallons per minute (from about 0.04 to about 1.9 lpm).9. The method of claim 1 where in the grinding the particulate polymer drag reducing agent has an average particle size of about 600 microns or less.10. The method of claim 1 where the feeding and grinding are conducted in the absence of cryogenic temperatures.11. The method of claim 1 where the feeding and grinding are conducted at ambient temperatures.12. A method for producing a particulate polymer drag reducing agent, comprising:feeding to a mill components comprising: granulated polymer; at least one solid organic grinding aid; and at least one liquid grinding aid; and grinding the components to produce at least 90 wt. % of the particulate polymer drag reducing agent having a size of about 600 microns or less, where the feeding and grinding are conducted in the absence of cryogenic temperatures. 13. The method of claim 12 where in the feeding, the granulated polymer is poly(alpha-olefin).14. The method of claim 12 where in the feeding, the solid organic grinding aid has a size between about 1 and about 50 microns.15. The method of claim 12 where in the feeding, the solid organic grinding aid is selected from the group consisting of ethene/butene copolymer, paraffin waxes, solid alcohols, and mixtures thereof.16. The method of claim 12 where in the feeding, the liquid grinding aid is a blend of at least one glycol selected from the group consisting of ethylene glycol, propylene glycol, diethylene glycol, dipropylene glycol, methyl ethers of such glycols, and mixtures thereof, and at least one other liquid selected from the group consisting of water and at least one alcohol, the alcohol being selected from the group consisting of methanol, ethanol, isopropanol and mixtures thereof.17. The method of claim 12 where in the feeding, the liquid grinding aid is a blend of glycol, water and isopropyl alcohol where the proportions range from about 20 to 80 wt. % to about 20 to 80 wt. % to about 0 to 30 wt. %.18. The method of claim 12 where in the feeding, the granulated polymer is fed at a rate of from about 100 to about 300 lbs/hr (45-138 kg/hr) the solid organic grinding aid is fed at a rate of from about 10 to about 90 lbs/hr (4.5-41 kg/hr) and the liquid grinding aid is fed at a rate of from about 0.01 to about 0.5 gallons per minute (from about 0.04 to about 1.9 lpm).19. A particulate polymer drag reducing agent (DRA) produced by a method comprising:feeding to a mill components comprising: granulated polymer; at least one solid organic grinding aid; and a liquid grinding aid; and grinding the components to produce particulate polymer drag reducing agent. 20. The particulate polymer DRA of claim 19 where in the feeding, the granulated polymer has a size between about 8 mm and about 12 mm.21. The particulate polymer DRA of claim 19 where in the feeding, the granulated polymer is poly(alpha-olefin).22. The particulate polymer DRA of claim 19 where in the feeding, the solid organic grinding aid has a size between about 1 and about 50 microns.23. The particulate polymer DRA of claim 19 where in the feeding, the solid organic grinding aid is selected from the group consisting of ethene/butene copolymer, paraffin waxes, solid alcohols, and mixtures thereof.24. The particulate polymer DRA of claim 19 where in the feeding, the liquid grinding aid is a blend of at least one glycol selected from the group consisting of ethylene glycol, propylene glycol, diethylene glycol, dipropylene glycol, methyl ethers of such glycols, and mixtures thereof, and at least one other liquid selected from the group consisting of water and at least one alcohol, the alcohol being selected from the group consisting of methanol, ethanol, isopropanol and mixtures thereof.25. The particulate polymer DRA of claim 19 where in the feeding, the liquid grinding aid is a blend of ethylene glycol, water and isopropanol where the proportions range from about 20 to 80 wt. % to about 20 to 80 wt. % to about 0 to 30 wt. %.26. The particulate polymer DRA of claim 19 where in the feeding, the granulated polymer is fed at a rate of from about 100 to about 300 lbs/hr (45-136 kg/hr) the solid organic grinding aid is fed at a rate of from about 10 to about 90 lbs/hr (4.5-41 kg/hr) and the liquid grinding aid is fed at a rate of from about 0.01 to about 0.5 gallons per minute (from about 0.04 to about 1.9 lpm).27. The particulate polymer DRA of claim 19 where in the grinding the particulate polymer drag reducing agent has an average particle size of about 600 microns or less.28. The particulate polymer DRA of claim 19 where the feeding and grinding are conducted in the absence of cryogenic temperatures.29. The particulate polymer DRA of claim 19 where the feeding and grinding are conducted at ambient temperatures.30. A particulate polymer drag reducing agent (DRA) produced by a method comprising:feeding to a mill components comprising: granulated polymer; at least one solid organic grinding aid; and at least one liquid grinding aid; and grinding the components to produce at least 90 wt % of the particulate polymer drag reducing agent having a size of about 600 microns or less, where the feeding and grinding are conducted in the absence of cryogenic temperatures. 31. The particulate polymer DRA of claim 30 where in the feeding, the granulated polymer is poly(alpha-olefin).32. The particulate polymer DRA of claim 30 where in the feeding, the solid organic grinding aid has a size between about 1 and about 50 microns.33. The particulate polymer DRA of claim 30 where in the feeding, the solid organic grinding aid is selected from the group consisting of ethene/butene copolymer, paraffin waxes, solid alcohols, and mixtures thereof.34. The particulate polymer DRA of claim 30 where in the feeding, the liquid grinding aid is a blend of at least one glycol selected from the group consisting of ethylene glycol, propylene glycol, diethylene glycol, dipropylene glycol, methyl ethers of such glycols, and mixtures thereof, and at least one other liquid selected from the group consisting of water and at least one alcohol, the alcohol being selected from the group consisting of methanol, ethanol, isopropanol and mixtures thereof.35. The particulate polymer DRA of claim 30 where in the feeding, the liquid grinding aid is a blend ethylene glycol, water and isopropanol where the proportions range from about 20 to 80 wt. % to about 20 to 80 wt. % to about 0 to 30 wt. %.36. The particulate polymer DRA of claim 30 where in the feeding, the granulated polymer is fed at a rate of from about 100 to about 300 lbs/hr (45-136 kgs/hr) the solid organic grinding aid is fed at a rate of from about 10 to about 90 lbs/hr (4.5-41 kg/hr) and the liquid grinding aid is fed at a rate of from about 0.01 to about 0.5 gallons per minute (from about 0.04 to about 1.9 lpm).37. A method of reducing drag in a hydrocarbon stream comprising:producing a particulate polymer drag reducing agent, comprising: feeding to a mill components comprising: granulated polymer; at least one solid organic grinding aid; and a liquid grinding aid; and grinding the components to produce particulate polymer drag reducing agent; and introducing the particulate polymer drag reducing agent into the hydrocarbon stream. 38. A method for producing a particulate polymer drag reducing agent, comprising:feeding to a mill components comprising: granulated polymer; and at least one solid organic grinding aid having a size between about 1 and about 50 microns; and grinding the components to produce particulate polymer drag reducing agent. 39. A particulate polymer drag reducing agent (DRA) produced by a method comprising:feeding to a mill components comprising: granulated polymer; at least one solid organic grinding aid having a size between about 1 and about 50 microns; and grinding the components to produce particulate polymer drag reducing agent. 40. A method of reducing drag in a hydrocarbon stream comprising:producing a particulate polymer drag reducing agent, comprising: feeding to a mill components comprising: granulated polymer; at least one solid organic grinding aid having a size between about 1 and about 50 microns; and grinding the components to produce particulate polymer drag reducing agent; and introducing the particulate polymer drag reducing agent into the hydrocarbon stream.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.