초록
▼
Cement compositions with improved mechanical properties and associated methods are provided, which are useful in conjunction with subterranean well operations. In certain embodiments, the cement compositions comprise carbon fibers, rubber particles, a hydraulic cement material, sufficient water to f
Cement compositions with improved mechanical properties and associated methods are provided, which are useful in conjunction with subterranean well operations. In certain embodiments, the cement compositions comprise carbon fibers, rubber particles, a hydraulic cement material, sufficient water to form a pumpable slurry, and optionally other ingredients including a dispersant, a weighting agent, a retarding or accelerating agent, or the like.
대표청구항
▼
1. A method of cementing in a subterranean formation comprising the steps of:providing a cement composition comprising a hydraulic cement, rubber particles, and carbon fibers; placing the cement composition in the subterranean formation; and allowing the cement composition to set therein. 2. The met
1. A method of cementing in a subterranean formation comprising the steps of:providing a cement composition comprising a hydraulic cement, rubber particles, and carbon fibers; placing the cement composition in the subterranean formation; and allowing the cement composition to set therein. 2. The method of claim 1 wherein the hydraulic cement is selected from the group consisting of Portland cements, pozzolana cements, gypsum cements, high alumina content cements, silica cements, and high alkalinity cements.3. The method of claim 1 wherein the hydraulic cement comprises a calcium phosphate cement.4. The method of claim 1 wherein the rubber particles are present in an amount of about 5% to about 50% by weight of the hydraulic cement in the composition.5. The method of claim 1 wherein the carbon fibers are present in an amount of about 1% to about 15% by weight of the hydraulic cement in the composition.6. The method of claim 1 wherein the rubber particles have a mean length of about ¼ inch or less.7. The method of claim 1 wherein the carbon fibers have a mean length of about 150 microns.8. The method of claim 1 wherein the cement composition further comprises an additive wherein the additive is a dispersant, a retardant, an accelerant, a fluid loss agent, a weighting agent, or a mixture thereof.9. The method of claim 1 wherein the cement composition has a tensile strength greater than 60 psi.10. The method of claim 1 wherein the rubber particles have a mean length of about ¼ inch or less and are present in an amount of about 5% to about 50% by weight of the hydraulic cement in the composition, and wherein the carbon fibers have a mean length of about 150 microns and are present in an amount of about 1% to about 15% by weight of the hydraulic cement in the composition.11. A method of increasing the tensile strength of a cement composition comprising rubber particles comprising the step of adding carbon fibers to the cement composition wherein the carbon fibers have a mean length of about 1 mm or less.12. The method of claim 11 wherein the carbon fibers are present in an amount of about 1% to about 15% by weight of a cement component of the cement composition.13. The method of claim 11 wherein the rubber particles are present in an amount of about 5% to about 50% by weight of a cement component of the cement composition.14. The method of claim 11 wherein the cement composition comprises a hydraulic cement selected from the group consisting of Portland cements, pozzolana cements, gypsum cements, high alumina content cements, silica cements, high alkalinity cements and calcium phosphate cements.15. A method of cementing in a subterranean formation comprising the steps of:providing a cement composition comprising a hydraulic cement and carbon fibers, the carbon fibers having a mean length of about 1 mm or less; placing the cement composition in the subterranean formation; and allowing the cement composition to set therein. 16. The method of claim 15 wherein the cement composition further comprises rubber particles.17. The method of claim 16 wherein the rubber particles are present in an amount of about 5% to about 50% by weight of the hydraulic cement in the composition.18. The method of claim 16 wherein the rubber particles have a mean length of about ¼ inch or less.19. The method of claim 15 wherein the hydraulic cement is selected from the group consisting of Portland cements, pozzolana cements, gypsum cements, high alumina content cements, silica cements, high alkalinity cements and calcium phosphate cements.20. The method of claim 15 wherein the carbon fibers are present in an amount of about 1% to about 15% by weight of the hydraulic cement component of the cement composition.21. The method of claim 15 wherein the hydraulic cement comprises a calcium phosphate cement.22. The method of claim 15 wherein the carbon fibers have a mean length of about 50 microns to about 500 microns.23. The method of claim 15 wherein the carbon fibers have a mean length of about 100 microns to about 200 microns.24. The method of claim 15 wherein the cement composition further comprises an additive wherein the additive is a dispersant, a retardant, an accelerant, a fluid loss agent, a weighting agent, or a mixture thereof.25. The method of claim 15 wherein the cement composition has a tensile strength greater than 60 psi.