초록
▼
The invention relates to a transparent protective layer, in particular a scratchproof layer for glass and glass-ceramic, which is able to withstand high temperatures, has a smooth and dense surface, an attractive surface design and is preferably used for coating cooking plates. A protective layer ac
The invention relates to a transparent protective layer, in particular a scratchproof layer for glass and glass-ceramic, which is able to withstand high temperatures, has a smooth and dense surface, an attractive surface design and is preferably used for coating cooking plates. A protective layer according to the invention comprises at least one crystalline metal oxide layer which has at least one interlayer formed from an amorphous, thermally stable mixed oxide, the interlayer being arranged being sublayers of the metal oxide layer. A further protective layer according to the invention comprises at least one amorphous, thermally stable mixed oxide layer which has at least one interlayer formed from a crystalline metal oxide, the interlayer being arranged between the sublayers of the amorphous mixed oxide layer. The amorphous mixed oxide layer has at least two metallic components. The crystalline metal oxide layers preferably consist of yttrium-stabilized zirconium oxide, and the amorphous mixed oxide layers preferably consist of titanium/aluminum oxide.
대표청구항
▼
The invention claimed is: 1. A transparent protective layer for use on a body, comprising: at least one hard-material layer, wherein said at least one hard-material layer has a crystalline metal oxide, said at least one hard-material layer having said crystalline metal oxide with at least one inter
The invention claimed is: 1. A transparent protective layer for use on a body, comprising: at least one hard-material layer, wherein said at least one hard-material layer has a crystalline metal oxide, said at least one hard-material layer having said crystalline metal oxide with at least one interlayer, said at least one interlayer formed from an amorphous, thermally stable mixed oxide, said amorphous, thermally stable mixed oxide having a metal oxide, said metal oxide having at least two metallic components, wherein said at least one interlayer is formed from said amorphous, thermally stable mixed oxide being arranged between at least two sublayers of the at least one hard-material layer with said crystalline metal oxide. 2. A transparent protective layer for use on a body, which comprises: at least one hard-material layer, wherein said at least one hard-material layer comprises an amorphous, thermally stable mixed oxide, said at least one hard-material layer having said amorphous, thermally stable mixed oxide with at least one interlayer formed from a crystalline metal oxide, said amorphous, thermally stable mixed oxide having a metal oxide with at least two metallic components, said at least one interlayer formed from said crystalline metal oxide being arranged between sublayers of said at least one hard-material layer having said amorphous, thermally stable mixed oxide. 3. A transparent protective layer for use on a body which comprises at least one hard-material layer, wherein said at least one hard-material layer has at least two sublayers, a first sublayer of said at least two sublayers having an amorphous, thermally stable mixed oxide and at least two metallic components, a second sublayer of said at least two sublayers having a crystalline metal oxide. 4. The transparent protective layer as claimed in claim 1, wherein said hard-material layer has a thickness in a range of between 100 to 20,000 nm. 5. The transparent protective layer as claimed in claim 4, wherein said thickness is in a range from 10 to 500 nm. 6. The transparent protective layer as claimed in claim 1, wherein said hard-material layer has a thickness is in a range from 10 to 500 nm. 7. The transparent protective layer as claimed in claim 1, wherein said at least two sublayers have said crystalline metal oxide with said metal oxide in a thermally stable crystal phase. 8. The transparent protective layer as claimed in claim 7, wherein said at least two sublayers have said crystalline metal oxide, which comprises aluminum oxide in a thermally stable crystal phase. 9. The transparent protective layer as claimed in claim 7, wherein said at least two sublayers have said crystalline metal oxide, which comprises zirconium oxide in a thermally stable crystal phase. 10. The transparent protective layer as claimed in claim 9, further comprising a component admixed to said zirconium oxide to stabilize said thermally stable crystal phase. 11. The transparent protective layer as claimed in claim 10, wherein said component is selected from the group consisting of an oxide, a combination of oxides, yttrium oxide, calcium oxide, magnesium oxide, tantalum oxide, niobium oxide, scandium oxide, titanium oxide, an oxide from the group of the lanthanoid oxides, lanthanum oxide, and cerium oxide. 12. The transparent protective layer as claimed in claim 9, wherein said at least two sublayers are said zirconium oxide, and wherein said at least one interlayer is said zirconium oxide with hafnium oxide. 13. The transparent protective layer as claimed in claim 11, wherein said at least two sublayers are said zirconium oxide, and wherein said at least one interlayer is said zirconium oxide with said component consisting of from 0.5 to 50 mol % of Y2O3. 14. The transparent protective layer as claimed in claim 13, wherein said at least two sublayers are said zirconium oxide, and wherein said at least one interlayer is said zirconium oxide with 4 mol % (짹1 mol %) of Y2O3 as said component. 15. A transparent protective layer for use on a body which comprises at least one hard-material layer, wherein said at least one hard-material layer has at least two sublayers with a first sublayer having an amorphous, thermally stable mixed oxide with at least two metallic components and a second sublayer with silicon nitride. 16. The transparent protective layer as claimed in claim 1, wherein at least one sublayer of said at least two sublayers has said amorphous, thermally stable mixed oxide with approximately a same refractive index as a second sublayer of the at least two sublayers with said crystalline metal oxide. 17. The transparent protective layer as claimed in claim 16, wherein said refractive index n of said at least one interlayer has said amorphous, thermally stable mixed oxide, and wherein at least one sublayer of said at least two sublayers has said amorphous, thermally stable mixed oxide varied using a quantitative ratio of said at least two metallic components. 18. The transparent protective layer as claimed in claim 1, wherein said at least one interlayer has said amorphous, thermally stable mixed oxide, and wherein at least one sublayer of said at least two sublayers has said amorphous, thermally stable mixed oxide with said at least two metallic components selected from the group consisting of Li, Be, Na, Mg, Al, Si, Ca, Sc, Ti, Cr, Zn, Ge, Sr, Y, Zr, Nb, Cd, In, Sn, Sb, Te, La, Ce, Pr, Nd, Sm, Gd, Yb, Lu, Hf, Ta, Tl, Pb, Bi, and Th. 19. The transparent protective layer as claimed in claim 17, wherein said at least one interlayer has said amorphous, thermally stable mixed oxide, and wherein at least one sublayer of said at least two sublayers has said amorphous, thermally stable mixed oxide with a titanium/aluminum oxide. 20. The transparent protective layer as claimed in claim 19, wherein said titanium/aluminum oxide is TixAl1-xO y, where 0<x<1. 21. The transparent protective layer as claimed in claim 20, wherein said refractive index n of said titanium/aluminum oxide is set in a range between 1.55≦n≦2.50 by a titanium to aluminum quantitative ratio. 22. The transparent protective layer as claimed in claim 1, further comprising a further transparent hard-material layer. 23. The transparent protective layer as claimed in claim 22, wherein said transparent hard-material layer has said amorphous, thermally stable mixed oxide, with said at least two metallic components. 24. The transparent protective layer as claimed in claim 23, wherein said transparent hard-material layer has the same components as said at least one interlayer and has the same components as at least one sublayer of said at least two sublayers. 25. The transparent protective layer as claimed in claim 22, wherein said transparent hard-material layer is said crystalline metal oxide. 26. The transparent protective layer as claimed in claim 25, wherein said transparent hard-material layer has the same components as said at least one interlayer with said crystalline metal oxide, and wherein said transparent hard material layer has the same components as at least one sublayer of said at least two sublayers. 27. The transparent protective layer as claimed in claim 22, wherein said transparent hard-material layer has a component selected from the group consisting of silicon oxide, and aluminum oxide. 28. The transparent protective layer as claimed in claim 22, wherein said transparent hard-material layer comprises silicon nitride. 29. The transparent protective layer as claimed in claim 1, wherein the transparent protective layer has a surface roughness with an Ra value of <50 nm. 30. The transparent protective layer as claimed in claim 1, wherein the transparent protective layer can be produced using a process selected from the group consisting of a CVD process, and a PVD process. 31. The transparent protective layer as claimed in claim 30, wherein the transparent protective layer is produced using a reactive PVD process. 32. The transparent protective layer as claimed in claim 31, wherein the transparent protective layer can be produced using a reactive sputtering process. 33. The transparent protective layer as claimed in claim 31, wherein the transparent protective layer forms a coating, wherein said coating is produced using a reactive ion beam-assisted PVD process. 34. The transparent protective layer as claimed in claim 33, wherein said coating is used for coating bodies made from a material selected from the group consisting of glass, glass-ceramic, non-metallic, crystalline materials, plastic bodies, and any combinations thereof. 35. The transparent protective layer as claimed in claim 1, wherein the transparent protective layer is coated on the body. 36. The transparent protective layer as claimed in claim 1, wherein the transparent protective layer is coated to a cooking hob. 37. The transparent protective layer as claimed in claim 1, wherein the transparent protective layer is coated to a cooking appliance.