IPC분류정보
국가/구분 |
United States(US) Patent
등록
|
국제특허분류(IPC7판) |
|
출원번호 |
US-0670149
(2008-07-25)
|
등록번호 |
US-8157051
(2012-04-17)
|
우선권정보 |
FR-07 05430 (2007-07-25) |
국제출원번호 |
PCT/FR2008/051402
(2008-07-25)
|
§371/§102 date |
20100421
(20100421)
|
국제공개번호 |
WO2009/016321
(2009-02-05)
|
발명자
/ 주소 |
- Marcel, Valérie
- Deshayes, Guillaume
|
출원인 / 주소 |
- Faurecia Automotive Industrie
|
대리인 / 주소 |
|
인용정보 |
피인용 횟수 :
7 인용 특허 :
7 |
초록
▼
This method includes the placing of the first porous layer (1) onto one part of a wall of a mold cavity having the shape desired by the soundproofing component, the first layer (1) not occupying the entire cavity, and the injection of a foaming polymer composition into the cavity of the mold to form
This method includes the placing of the first porous layer (1) onto one part of a wall of a mold cavity having the shape desired by the soundproofing component, the first layer (1) not occupying the entire cavity, and the injection of a foaming polymer composition into the cavity of the mold to form the second open-cell porous layer (3). The two steps of placing the practically airtight intermediate layer (2) onto the first porous layer (1) and of injecting a polymer composition in order to form the second porous layer (3) are carried out simultaneously in a single step of injecting the foaming polymer composition.
대표청구항
▼
1. A method for producing a moulded sound-proofing component comprising a first porous layer and a second porous layer having open cells with an intermediate layer that is practically air-tight provided therebetween, the method comprising: providing the first porous layer having a shape provided by
1. A method for producing a moulded sound-proofing component comprising a first porous layer and a second porous layer having open cells with an intermediate layer that is practically air-tight provided therebetween, the method comprising: providing the first porous layer having a shape provided by the sound-proofing component;providing the intermediate layer on the first porous layer; andinjecting a polymer foaming composition to form the second porous layer,wherein the providing the intermediate layer on the first porous layer and the injecting a polymer foaming composition are carried out simultaneously in a single injection step of the polymer foaming composition to contact the first layer during formation of a polymer composition from the polymer foaming composition and the material of the first layer, and the intermediate layer being denser than each of the first and second porous layers,wherein the providing the first layer includes providing a layer of a porous material, the porous material being selected from a felt and a foam layer, and the first porous layer consists of one porous layer having a resistance to passage of air of between 200 N·m−3·s and 3500 N·m−3·s, andwherein a density of the intermediate layer is lower the 666 kg/m3. 2. The method according to claim 1, wherein the thickness of the intermediate layer after injection is between 10% and 20% of the thickness of the first porous layer. 3. The method according to claim 1, wherein the intermediate layer has a mass per unit area of between 100 g/m2 and 1000 g/m2. 4. The method according to claim 1, wherein the intermediate layer and the second porous layer are produced in such a manner that the polymer foaming composition injected in order to form the second porous layer penetrates into the porous structure of the first porous layer. 5. A moulded sound-proofing component produced by the method according to claim 1, wherein the intermediate layer is constituted only by the materials of the first and second porous layers. 6. The sound-proofing component according to claim 5, wherein the thickness of the intermediate layer is between 10% and 20% of the thickness of the first porous layer. 7. The sound-proofing component according to claim 5, wherein the intermediate layer has a mass per unit area of between 100 g/m2 and 1000 g/m2. 8. The sound-proofing component according to claim 5, wherein the first porous layer is provided with a porous layer whose external surface carries an additional layer having greater resistance to passage of air. 9. The sound-proofing component according to claim 8, wherein the additional layer having the greater resistance to passage of air has a resistance to passage of air of between 200 N·m−3·s and 2000 N·m−3·s. 10. The sound-proofing component according to claim 5, further comprising a decorative matting layer provided on the first porous layer with a fine fluid-tight film being interposed therebetween. 11. The method according to claim 1, wherein the porous material of the first layer is provided with a porous layer whose external surface carries an additional layer having greater resistance to passage of air, and the step of providing the first layer comprises the positioning of the first layer of the porous material in such a manner that the additional layer having the greater resistance to passage of air is positioned at an exterior of the moulded sound-proofing component. 12. The sound-proofing component according to claim 6, wherein the intermediate layer has a mass per unit area of between 100 g/m2 and 1000 g/m2. 13. A method for producing a moulded sound-proofing component comprising a first porous layer and a second porous layer having open cells with an intermediate layer that is practically air-tight provided therebetween, the method comprising: providing the first porous layer having a shape provided by the sound-proofing component;providing the intermediate layer on the first porous layer; andinjecting a polymer foaming composition to form the second porous layer,wherein the providing the intermediate layer on the first porous layer and the injecting a polymer foaming composition are carried out simultaneously in a single injection step of the polymer foaming composition contacting the first layer during formation of a polymer composition from the polymer foaming composition and the material of the first layer, and the intermediate layer being denser than each of the first and second porous layers,wherein the providing the first layer includes providing a layer of a porous material, the porous material being selected from a felt and a foam layer,wherein the porous material of the first layer is provided with a porous layer whose external surface carries an additional layer having greater resistance to passage of air, and the step of providing the first layer includes the providing of the layer of the porous material in such a manner that the additional layer having the greater resistance to passage of air is positioned at an exterior of the moulded sound-proofing component,wherein the additional layer having the greater resistance to passage of air has a resistance to passage of air of between 200 N·m−3·s and 2000 N·m−3·s, andwherein a density of the intermediate layer is lower the 666 kg/m3. 14. The method according to claim 13, wherein the intermediate layer has a mass per unit area of between 100 g/m2 and 1000 g/m2. 15. The method according to claim 13, wherein the intermediate layer and the second porous layer are produced in such a manner that the polymer foaming composition injected in order to form the second porous layer penetrates into the porous structure of the first porous layer. 16. A moulded sound-proofing component produced by the method according to claim 13, wherein the intermediate layer is constituted only by the materials of the first and second porous layers. 17. The sound-proofing component according to claim 16, wherein the thickness of the intermediate layer is between 10% and 20% of the thickness of the first porous layer. 18. The sound-proofing component according to claim 16, wherein the intermediate layer has a mass per unit area of between 100 g/m2 and 1000 g/m2. 19. The sound-proofing component according to claim 16, further comprising a decorative matting layer provided on the first porous layer with a fine fluid-tight film being interposed therebetween. 20. A method for producing a moulded sound-proofing component comprising a first porous layer and a second porous layer having open cells with an intermediate layer that is practically air-tight provided therebetween, the method comprising: providing the first porous layer having a shape provided by the sound-proofing component;providing the intermediate layer on the first porous layer; andinjecting a polymer foaming composition to form the second porous layer,wherein the providing the intermediate layer on the first porous layer and the injecting a polymer foaming composition are carried out simultaneously in a single injection step of the polymer foaming composition to contact the first layer during formation of a polymer composition from the polymer foaming composition and the material of the first layer, and the intermediate layer being denser than each of the first and second porous layers,wherein the providing the first layer includes providing a layer of a porous material, the porous material being selected from a felt and a foam layer, and the first porous layer consists of one porous layer having a resistance to passage of air of between 200 N·m−3·s and 3500 N·m−3·s,wherein a density of the intermediate layer is lower the 666 kg/m3, andwherein the resulting moulded sound-proofing component comprising the first porous layer and the second porous layer having open cells with the intermediate layer that is practically air-tight provided therebetween is configured as one of a motor vehicle floor sound-proofing component and a motor vehicle bulkhead sound-proofing component.