Stainless steel excellent in corrosion resistance, ferritic stainless steel excellent in resistance to crevice corrosion and formability, and ferritic stainless steel excellent in resistance to crevice corrosion
원문보기
The stainless steel of the first embodiment includes C: 0.001 to 0.02%, N: 0.001 to 0.02%, Si: 0.01 to 0.5%, Mn: 0.05 to 0.5%, P: 0.04% or less, S: 0.01% or less, Ni: more than 3% to 5%, Cr: 11 to 26%, and either one or both of Ti: 0.01 to 0.5% and Nb: 0.02 to 0.6%, and contains as the remainder, Fe
The stainless steel of the first embodiment includes C: 0.001 to 0.02%, N: 0.001 to 0.02%, Si: 0.01 to 0.5%, Mn: 0.05 to 0.5%, P: 0.04% or less, S: 0.01% or less, Ni: more than 3% to 5%, Cr: 11 to 26%, and either one or both of Ti: 0.01 to 0.5% and Nb: 0.02 to 0.6%, and contains as the remainder, Fe and unavoidable impurities. The stainless steel of the second embodiment has an alloy composition different from those of the first and third embodiments and satisfies the formula (A): Cr+3Mo+6Ni≧23 and formula (B): Al/Nb≧10 and contains as the remainder, Fe and unavoidable impurities. The stainless steel of the third embodiment has an alloy composition different from those of the first and second embodiments and includes either one or both of Sn: 0.005 to 2% and Sb: 0.005 to 1% and contains as the remainder, Fe and unavoidable impurities.
대표청구항▼
1. A ferritic stainless steel consisting of, in terms of mass %, C: 0.001 to 0.02%, N: 0.001 to 0.02%, Si: 0.01 to 0.5%, Mn: 0.05 to 1%, P: 0.04% or less, S: 0.01% or less, Cr: 12 to 25%, Ti: 4(C+N) to 0.5%, B: 0.0002 to 0.0004%, Sn: 0.01 to 2%, andoptionally, one or more of Sb: 0.005 to 1%, Nb: 0.0
1. A ferritic stainless steel consisting of, in terms of mass %, C: 0.001 to 0.02%, N: 0.001 to 0.02%, Si: 0.01 to 0.5%, Mn: 0.05 to 1%, P: 0.04% or less, S: 0.01% or less, Cr: 12 to 25%, Ti: 4(C+N) to 0.5%, B: 0.0002 to 0.0004%, Sn: 0.01 to 2%, andoptionally, one or more of Sb: 0.005 to 1%, Nb: 0.02 to 1%, Ni: 0.2 to 5%, Cu: 1.5% or less, W: 5% or less, Al: 1% or less, and Ca: 0.002% or less,with a remainder of Fe and unavoidable impurities. 2. A ferritic stainless steel consisting of, in terms of mass %, C: 0.001 to 0.02%, N: 0.001 to 0.02%, Si: 0.01 to 0.5%, Mn: 0.05 to 1%, P: 0.04% or less, S: 0.01% or less, Cr: 12 to 25%, Ti: 4(C+N) to 0.5%, B: 0.0002 to 0.0004%, Sn: 0.01 to 2%, andoptionally, one or more of Sb: 0.005 to 1%, Nb: 0.02 to 1%, Ni: 0.2 to 5%, Cu: 1.5% or less, W: 5% or less, Al: 1% or less, and Ca: 0.002% or less,with a remainder of Fe and unavoidable impurities, andwherein a critical passivation current density is 2.3 mA/cm2 or less. 3. A ferritic stainless steel consisting of, in terms of mass %, C: 0.001 to 0.02%, N: 0.001 to 0.02%, Si: 0.01 to 0.5%, Mn: 0.05 to 1%, P: 0.04% or less, S: 0.01% or less, Cr: 12 to 25%, Ti: 4(C+N) to 0.5%, B: 0.0002 to 0.0004%, Sn: 0.01 to 2%, andoptionally, one or more of Sb: 0.005 to 1%, Nb: 0.02 to 1%, Ni: 0.2 to 5%, Cu: 1.5% or less, W: 5% or less, Al: 1% or less, and Ca: 0.002% or less,with a remainder of Fe and unavoidable impurities, andwherein a maximum value for corrosion depth is 600 μm or less which is measured by a corrosion testing method for automobile materials in conformity with JASO M609-91. 4. The ferritic stainless steel of claim 3, wherein a critical passivation current density is 2.3 mA/cm2 or less.
연구과제 타임라인
LOADING...
LOADING...
LOADING...
LOADING...
LOADING...
이 특허에 인용된 특허 (8)
Oppenheim Rudolf (Krefeld DEX) Kiesheyer Heinrich (Krefeld DEX) Brandis Helmut (Krefeld DEX) Lennartz Gustav (Krefeld DEX) Thielmann Rainer (Krefeld DEX), Corrosion-resistant ferritic chrome-molybdenum-nickel steel.
Hatano, Masaharu; Ishimaru, Eiichiro; Takahashi, Akihiko; Kimura, Ken; Teraoka, Shinichi, Ferritic stainless steel plate which has excellent ridging resistance and method of production of same.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.