초록
Demineralized bone particles are obtained by demineralizing whole bone and thereafter subdividing the demineralized bone to provide the demineralized bone particles.
대표청구항
▼
1. A method of making demineralized bone particles, comprising: demineralizing whole bone, the whole bone comprising collagen fibers; and thereafter subdividing the demineralized bone by pressing the demineralized bone into demineralized bone particles comprising intact collagen fibers, wherein pres
1. A method of making demineralized bone particles, comprising: demineralizing whole bone, the whole bone comprising collagen fibers; and thereafter subdividing the demineralized bone by pressing the demineralized bone into demineralized bone particles comprising intact collagen fibers, wherein pressing the demineralized bone comprises applying a mechanical pressure to the demineralized bone from about 1,000 to about 40,000 psi. 2. The method as recited in claim 1, wherein the intact collagen fibers are not joined from fiber sections. 3. The method as recited in claim 1, wherein at least one of the intact collagen fibers has a length equal to at least one of the collagen fibers of the whole bone. 4. The method as recited in claim 1, wherein the intact collagen fibers range in length from 10-15 mm. 5. The method as recited in claim 1, wherein the intact collagen fibers range in length from 20-25 mm. 6. The method as recited in claim 1, wherein pressing the demineralized bone into demineralized bone particles comprises: performing a first pressing by applying pressure ranging from about 5,000 to about 20,000 psi; andperforming a second pressing by applying pressure ranging from 5,000 to about 10,000 psi. 7. The method as recited in claim 1, wherein pressing the demineralized bone comprises pressing the demineralized bone between two plates of a Carver press. 8. The method as recited in claim 1, wherein pressing the demineralized bone comprises applying a pressure from about 5,000 to about 20,000 psi. 9. The method as recited in claim 1, wherein demineralizing the whole bone comprises defatting the whole bone in an aqueous solution of ethanol, the solution comprising about 60% to about 90% alcohol by weight. 10. The method as recited in claim 1, wherein demineralizing the whole bone comprises defatting the whole bone in a solution of comprising Triton X-100 at a concentration of 0.1% to 10% in water. 11. The method as recited in claim 1, wherein demineralizing the whole bone comprises immersing the whole bone in peracetic acid. 12. The method as recited in claim 1, wherein a yield of demineralized bone particles is greater than that obtained by subdividing the whole bone into mineralized bone particles and thereafter demineralizing the mineralized bone particles to provide demineralized bone particles. 13. The method as recited in claim 1, wherein at least about 80 weight percent of the particles have a median length to width ratio of from about 2 to 200. 14. A method of making demineralized bone particles, comprising: demineralizing whole bone, the whole bone comprising collagen fibers; and thereafter subdividing the demineralized bone by pressing the demineralized bone into demineralized bone particles comprising intact collagen fibers,wherein at least one of the intact collagen fibers have a length equivalent to that of at least one of the collagen fibers of the whole bone and the demineralized bone particles are separated into bone collagen bundles, wherein pressing the demineralized bone comprises applying a mechanical pressure to the demineralized bone from about 1,000 to about 40,000 psi. 15. A method of making demineralized bone particles, comprising: demineralizing whole bone, the whole bone comprising collagen fibers; thereafter subdividing the demineralized bone by pressing the demineralized bone into demineralized bone particles comprising intact collagen fibers, wherein pressing the demineralized bone comprises applying a mechanical pressure to the demineralized bone from about 1,000 to about 40,000 psi; andforming the demineralized bone particles into one of a gel, a putty or a sheet. 16. The method as recited in claim 15, further comprising admixing the demineralized bone particles with at least one selected from the group consisting of adhesives, fillers, plasticizers, flexibilizing agents, biostatic/biocidal agents, surface active agents, and binding/bonding agents. 17. The method as recited in claim 15, further comprising admixing the demineralized bone particles with at least one selected from the group consisting of acrylic resins, cellulosics, bioresorbable polymers, polyesters, polycarbonates, polyarylates, polyfumarates, tyrosine polycarbonates, tyrosine polyarylates, polyglycolides, polylactides, glycolide-lactide copolymer, bone powder, demineralized bone powder, hydroxyapatite, liquid polyhydroxy compounds, glycerol, monacetin, diacetin, antibiotics, providone, sugars, and amphoteric surfactants. 18. The method as recited in claim 15, wherein the demineralized bone particles are formed into a sheet.