IPC분류정보
국가/구분 |
United States(US) Patent
등록
|
국제특허분류(IPC7판) |
|
출원번호 |
US-0218525
(2011-08-26)
|
등록번호 |
US-8808633
(2014-08-19)
|
우선권정보 |
WO-PCT/JP2010/065050 (2010-09-02) |
발명자
/ 주소 |
- Kunieda, Masafumi
- Matsukawa, Yosuke
- Murakami, Takunari
|
출원인 / 주소 |
|
대리인 / 주소 |
|
인용정보 |
피인용 횟수 :
2 인용 특허 :
1 |
초록
▼
A silico-alumino phosphate includes Si, Al, and P. A ratio of an amount of substance of Si to a sum of an amount of substance of Al and an amount of substance of P is approximately 0.22 or more and approximately 0.33 or less. An acid point is approximately 1.2 mmol/g or more. A honeycomb structural
A silico-alumino phosphate includes Si, Al, and P. A ratio of an amount of substance of Si to a sum of an amount of substance of Al and an amount of substance of P is approximately 0.22 or more and approximately 0.33 or less. An acid point is approximately 1.2 mmol/g or more. A honeycomb structural body includes a honeycomb unit. The honeycomb unit includes the silico-alumino phosphate and an inorganic binder. The honeycomb unit has a plurality of through-holes divided by a plurality of partition walls and arranged in a longitudinal direction of the honeycomb unit. An exhaust gas conversion apparatus includes the honeycomb structural body, a holding sealing member and a metal pipe. The holding sealing member is provided at an outer peripheral portion of the honeycomb structural body. The honeycomb structural body and the holding sealing member are installed in the metal pipe.
대표청구항
▼
1. A silico-alumino phosphate comprising: Si;Al; andP, a ratio of an amount of substance of Si to a sum of an amount of substance of Al and an amount of substance of P being approximately 0.22 or more and approximately 0.33 or less, an acid point being approximately 1.2 mmol/g or more. 2. The silico
1. A silico-alumino phosphate comprising: Si;Al; andP, a ratio of an amount of substance of Si to a sum of an amount of substance of Al and an amount of substance of P being approximately 0.22 or more and approximately 0.33 or less, an acid point being approximately 1.2 mmol/g or more. 2. The silico-alumino phosphate as claimed in claim 1, wherein the silico-alumino phosphate is ion-exchanged with at least one of a copper ion and an iron ion. 3. The silico-alumino phosphate as claimed in claim 1, wherein the ratio of the amount of substance of Si to the sum of the amount of substance of Al and the amount of substance of P is approximately 0.26 or more and approximately 0.33 or less. 4. The silico-alumino phosphate as claimed in claim 1, wherein an upper limit of the acid point of the silico-alumino phosphate is a theoretical value calculated from a formula (A) the theoretical value=(ratio of the amount of substance of Si to the sum of the amount of substance of Al and P)×12.9 [mmol/g] (A). 5. A honeycomb structural body comprising: a honeycomb unit including the silico-alumino phosphate as claimed in claim 1 and an inorganic binder, the honeycomb unit having a plurality of through-holes divided by a plurality of partition walls and arranged in a longitudinal direction of the honeycomb unit. 6. The honeycomb structural body as claimed in claim 5, wherein the silico-alumino phosphate forms a plurality of particles, and an average diameter of original particles of the plurality of particles is approximately 1 μm or more and approximately 5 μm or less. 7. The honeycomb structural body as claimed in claim 5, wherein the inorganic binder includes a solid containing at least one selected from a group of alumina sol, silica sol, titania sol, soluble glass, sepiolite, attapulgite, and boehmite. 8. The honeycomb structural body as claimed in claim 5, wherein the silico-alumino phosphate is ion-exchanged with at least one of a copper ion and an iron ion. 9. The honeycomb structural body as claimed in claim 8, wherein the silico-alumino phosphate is ion-exchanged with at least one of a copper ion and an iron ion, and an ion exchange amount is from approximately 1.0 to approximately 5.0 mass %. 10. The honeycomb structural body as claimed in claim 5, wherein the ratio of the amount of substance of Si to the sum of the amount of substance of Al and the amount of substance of P is approximately 0.26 or more and approximately 0.33 or less. 11. The honeycomb structural body as claimed in claim 5, wherein an upper limit of the acid point of the silico-alumino phosphate is a theoretical value calculated from a formula (A), the theoretical value=(ratio of the amount of substance of Si to the sum of the amount of substance of Al and P)×12.9 [mmol/g] (A). 12. The honeycomb structural body as claimed in claim 5, wherein the honeycomb unit includes at least one material selected from a group of an inorganic fiber, a scale-like material, a tetrapod-shaped material, and a three-dimensional needle-shaped material. 13. The honeycomb structural body as claimed in claim 12, wherein the inorganic fiber includes at least one selected from a group of alumina fiber, silica fiber, silicon carbide fiber, silica alumina fiber, glass fiber, potassium titanate fiber, and aluminum borate fiber,the scale-like material includes at least one selected from a group of glass, muscovite, alumina, and silica,the tetrapod-shaped material includes zinc oxide, andthe three-dimensional needle-shaped material includes at least one selected from alumina, silica, silicon carbide, silica alumina, glass, potassium titanate, aluminum borate, and boehmite. 14. The honeycomb structural body as claimed in claim 12, wherein a content of at least one selected from a group of the inorganic fiber, the scale-like material, tetrapod-shaped material, and the three-dimensional needle-like material in the honeycomb unit is from approximately 3 mass % to approximately 50 mass %. 15. The honeycomb structural body as claimed in claim 5, wherein a number of the honeycomb units is two or more. 16. The honeycomb structural body as claimed in claim 5, wherein a number of the honeycomb units is one. 17. The honeycomb structural body as claimed in claim 5, further comprising an outer peripheral coating layer formed on an outer peripheral surface of the honeycomb structural body. 18. The honeycomb structural body as claimed in claim 5, wherein a content of the silico-alumino phosphate by weight per apparent volume is from approximately 230 to approximately 360 g/L. 19. The honeycomb structural body as claimed in claim 5, wherein a content of the inorganic binder as a solid component in the honeycomb unit is from approximately 5 to approximately 30 mass %. 20. The honeycomb structural body as claimed in claim 5, wherein a porosity of the honeycomb unit is from approximately 25% to approximately 40%. 21. The honeycomb structural body as claimed in claim 5, wherein an aperture ratio of a cross section of the honeycomb unit perpendicular to the longitudinal direction of the honeycomb unit is from approximately 50% to approximately 75%. 22. The honeycomb structural body as claimed in claim 5, a density of the through-holes of a cross section perpendicular to the longitudinal direction of the honeycomb unit is from approximately 31 to approximately 155 units per cm2. 23. The honeycomb structural body as claimed in claim 5, wherein a thickness of each of the plurality of partition walls of the honeycomb unit is from approximately 0.10 mm to approximately 0.50 mm. 24. A honeycomb structural body comprising: a honeycomb unit including cordierite and having a plurality of through-holes divided by a plurality of partition walls and arranged in a longitudinal direction of the honeycomb unit, wherein the plurality of partition walls carry the silico-alumino phosphate of claim 1. 25. The honeycomb structural body as claimed in claim 24, wherein the silico-alumino phosphate is ion-exchanged with at least of one of a copper ion and an iron ion. 26. The honeycomb structural body as claimed in claim 24, wherein the ratio of the amount of substance of Si to the sum of the amount of substance of Al and the amount of substance of P is approximately 0.26 or more and approximately 0.33 or less. 27. The honeycomb structural body as claimed in claim 24, wherein an upper limit of the acid point of the silico-alumino phosphate is a theoretical value calculated from a formula (A), the theoretical value=(ratio of the amount of substance of Si to the sum of the amount of substance of Al and P)×12.9 [mmol/g]. (A). 28. The honeycomb structural body as claimed in claim 24, wherein the silico-alumino phosphate forms a plurality of particles, and an average diameter of original particles of the plurality of particles is approximately 1 μm or more and approximately 5 μm or less. 29. The honeycomb structural body as claimed in claim 24, wherein a number of the honeycomb units is one. 30. The honeycomb structural body as claimed in claim 24, further comprising an outer peripheral coating layer formed on an outer peripheral surface of the honeycomb structural body. 31. An exhaust gas conversion apparatus comprising: the honeycomb structural body as claimed in claim 24;a holding sealing member provided at an outer peripheral portion of the honeycomb structural body; anda metal pipe having the honeycomb structural body and the holding sealing member installed in the metal pipe. 32. The exhaust gas conversion apparatus as claimed in claim 31, wherein the silico-alumino phosphate is ion-exchanged with at least one of a copper ion and an iron ion. 33. The exhaust gas conversion apparatus as claimed in claim 31, wherein the ratio of the amount of substance of Si to the sum of the amount of substance of Al and the amount of substance of P is approximately 0.26 or more and approximately 0.33 or less. 34. The exhaust gas conversion apparatus as claimed in claim 31, wherein an upper limit of the acid point of the silico-alumino phosphate is a theoretical value calculated from a formula (A), The theoretical value=(ratio of the amount of substance of Si to the sum of the amount of substance of Al and P)×12.9 [mmol/g] (A). 35. The exhaust gas conversion apparatus as claimed in claim 31, wherein the silico-alumino phosphate has forms a plurality of particles, and an average diameter of original particles of the plurality of particle is approximately 1 μm or more and approximately 5 μm or less. 36. The exhaust gas conversion apparatus as claimed in claim 31, wherein a number of the honeycomb units is one. 37. The exhaust gas conversion apparatus as claimed in claim 31, further comprising an outer peripheral coating layer formed on an outer peripheral surface of the honeycomb structural body. 38. An exhaust gas conversion apparatus comprising: the honeycomb structural body as claimed in claim 5;a holding sealing member provided at an outer peripheral portion of the honeycomb structural body; anda metal pipe having the honeycomb structural body and the holding sealing member installed in the metal pipe. 39. The exhaust gas conversion apparatus as claimed in claim 38, wherein the silico-alumino phosphate forms a plurality of particles, and an average diameter of original particles of the plurality of particles is 1 μm or more and approximately 5 μm or less. 40. The exhaust gas conversion apparatus as claimed in claim 38, wherein the inorganic binder includes a solid containing at least one selected from a group of alumina sol, silica sol, titania sol, soluble glass, sepiolite, attapulgite, and boehmite. 41. The exhaust gas conversion apparatus as claimed in claim 38, wherein the silico-alumino phosphate is ion-exchanged with at least one of a copper ion and an iron ion. 42. The exhaust gas conversion apparatus as claimed in claim 38, wherein the ratio of the amount of substance of Si to the sum of the amount of substance of Al and the amount of substance of P is approximately 0.26 or more and approximately 0.33 or less. 43. The exhaust gas conversion apparatus as claimed in claim 38, wherein an upper limit of the acid point of the silico-alumino phosphate is a theoretical value calculated from a formula (A), the theoretical value=(ratio of the amount of substance of Si to the sum of the amount of substance of Al and P)×12.9 [mmol/g] (A). 44. The exhaust gas conversion apparatus as claimed in claim 38, wherein the silico-alumino phosphate is ion-exchanged with at least one of a copper ion and an iron ion, and an ion exchange amount is from approximately 1.0 to approximately 5.0 mass %. 45. The exhaust gas conversion apparatus as claimed in claim 44, wherein the inorganic fiber includes at least one selected from a group of alumina fiber, silica fiber, silicon carbide fiber, silica alumina fiber, glass fiber, potassium titanate fiber, and aluminum borate fiber,the scale-like material includes one least one selected from a group of glass, muscovite, alumina, and silica,the tetrapod-shaped material includes zinc oxide, andthe three-dimensional needle-shaped material includes at least one selected from alumina, silica, silicon carbide, silica alumina, glass, potassium titanate, aluminum borate, and boehmite. 46. The exhaust gas conversion apparatus as claimed in claim 45 wherein the honeycomb unit includes at least one material selected from a group of an inorganic fiber, a scale-like material, a tetrapod-shaped material, and a three-dimensional needle-shaped material. 47. The exhaust gas conversion apparatus as claimed in claim 38, wherein a number of the honeycomb units is two or more. 48. The exhaust gas conversion apparatus as claimed in claim 38, wherein a number of the honeycomb units is one. 49. The exhaust gas conversion apparatus as claimed in claim 38, further comprising an outer peripheral coating layer formed on an outer peripheral surface of the honeycomb structural body. 50. The exhaust gas conversion apparatus as claimed in claim 38, wherein a content of a silico-alumino phosphate by weight per apparent volume in the honeycomb unit is from approximately 230 to approximately 360 g/L. 51. The exhaust gas conversion apparatus as claimed in claim 38, wherein a content of the inorganic binder as a solid component of the honeycomb unit is from approximately 5 to approximately 30 mass %. 52. The exhaust gas conversion apparatus as claimed in claim 46, wherein a content of at least one selected from a group of the inorganic fiber, the scale-like material, the tetrapod-shaped material, and the three-dimensional needle-like material in the honeycomb unit is from approximately 3 mass % to approximately 50 mass %. 53. The exhaust gas conversion apparatus as claimed in claim 38, wherein a porosity of the honeycomb unit is from approximately 25% to approximately 40%. 54. The exhaust gas conversion apparatus as claimed in claim 38, wherein an aperture ratio of a cross section of the honeycomb unit perpendicular to the longitudinal direction of the honeycomb unit is from approximately 50% to approximately 75%. 55. The exhaust gas conversion apparatus as claimed in claim 38, a density of the through-holes of the cross section perpendicular to the longitudinal direction of the honeycomb unit is from approximately 31 to approximately 155 units per cm2. 56. The exhaust gas conversion apparatus as claimed in claim 38, wherein a thickness of each of the plurality of the partition walls of the honeycomb unit is from approximately 0.10 mm to approximately 0.50 mm.