Method for manufacturing an optical component for eliminating surface defects
IPC분류정보
국가/구분
United States(US) Patent
등록
국제특허분류(IPC7판)
B24B-001/00
B24B-037/04
B24B-013/00
B24B-051/00
B23K-026/00
C03B-029/02
C03C-019/00
C03C-023/00
B23K-026/03
출원번호
US-0129621
(2012-06-29)
등록번호
US-9138859
(2015-09-22)
우선권정보
FR-11 55971 (2011-07-01)
국제출원번호
PCT/FR2012/051506
(2012-06-29)
§371/§102 date
20131227
(20131227)
국제공개번호
WO2013/004955
(2013-01-10)
발명자
/ 주소
Cormont, Philippe
Rullier, Jean-Luc
출원인 / 주소
COMMISSARIAT A L'ENERGIE ATOMIQUE ET AUX ENERGIES ALTERNATIVES
대리인 / 주소
Young & Thompson
인용정보
피인용 횟수 :
0인용 특허 :
5
초록▼
Method for manufacturing an optical component, including a substrate made of a fusible material, includes the following steps a) and b) of steps a), b) and c), or steps a), b), c) and d): a) roughing; b) fine grinding; c) polishing; and d) finishing. The method includes steps, subsequent to any one
Method for manufacturing an optical component, including a substrate made of a fusible material, includes the following steps a) and b) of steps a), b) and c), or steps a), b), c) and d): a) roughing; b) fine grinding; c) polishing; and d) finishing. The method includes steps, subsequent to any one of steps b), c) and/or d): e) inspecting the optical surface of the optical component; f) detecting and locating at least one surface defect to be eliminated; g) for each surface defect, applying a laser beam to an area emcompassing the defect, so as to produce a local remelting of the fusible material, and to form, at the location of the defect, an area of material remelted; h) polishing the optical surface including at least one area of remelted material, to produce a polished optical surface free of surface defects, and continuing with steps c) and d).
대표청구항▼
1. A method of manufacturing an optical component (100) comprising a substrate made of a fusible material, said method comprising the following steps a) and b) or steps a), b) and c) or steps a), b), c) and d): a. Roughing (10) the optical component (100) to form at least one optical surface (110) o
1. A method of manufacturing an optical component (100) comprising a substrate made of a fusible material, said method comprising the following steps a) and b) or steps a), b) and c) or steps a), b), c) and d): a. Roughing (10) the optical component (100) to form at least one optical surface (110) on said substrate;b. Smooth grinding (20) said optical surface (110) of the optical component (100) so as to obtain a smoothed optical surface;c. Polishing (40) said smoothed optical surface so as to obtain a polished optical surface;d. Finishing (60) said polished optical surface so as to obtain a finished optical surface;wherein said method further comprises, after any one of steps b), and/or c), the following steps:e. Inspecting (30′, 50′, 70′) the smoothed or polished optical surface of the optical component to detect and locate at least one surface defect to be eliminated (120) on the smoothed or polished optical surface of the optical component;f. For each surface defect to be eliminated (120) located at step e), applying a laser beam (35, 55, 75) over an area encompassing said surface defect to be eliminated, said laser beam having a laser emission wavelength suitable for being absorbed by said material, so as to produce a local remelting of the fusible material, the power density of the laser beam and the duration of application of the laser beam being function of the transverse dimensions of the surface defect to be eliminated (120), so as to form, in place of the surface defect to be eliminated, an area of laser remelted material (310); andg. Continuing the method of manufacturing the optical component at step c) when step f) has been performed before the end of step c); or, respectively, at step d) when step f) has been performed after the end of step c). 2. The method of manufacturing an optical component (100) according to claim 1, wherein step e) of inspection (30′, 50′, 70′) of the optical surface of the optical component comprises a chemical etching. 3. The method of manufacturing an optical component (100) according to claim 1, wherein step e) of inspection (30′, 50′, 70′) comprises an optical measurement of scattering and/or diffraction. 4. The method of manufacturing an optical component (100) according to claim 1, wherein step e) of inspection (30′, 50′, 70′) comprises the detection and location of at least one surface defect (120) having a transverse dimension greater than or equal to 10 microns on the optical surface. 5. The method of manufacturing an optical component (100) according to claim 1, wherein step f) of application of a laser beam (35, 55, 75) comprises the application of a CO2 laser beam at a wavelength of 10.6 μm, said laser being continuous or pulsed. 6. The method of manufacturing an optical component (100) according to claim 1, wherein the fusible material is glass and step f) of application of a laser beam (35, 55, 75) causes an increase of the local temperature of the glass, said local temperature of the glass being comprised between 1000K and 2000K in an area encompassing said surface defect to be eliminated (120) located at step e). 7. The method of manufacturing an optical component (100) according to claim 1, wherein step f) is combined to a spatial sweep of the laser beam over the surface of the optical component along the surface defect to be eliminated (120). 8. The method of manufacturing an optical component (100) according to claim 1, wherein the polishing step (40) that follows step f) comprises a material removal over a thickness lower than the depth of the initial surface defect (120) and higher than or equal to the depth of the surface deformations of the area of laser remelted material (310) generated by step f) of application of the laser beam. 9. The method of manufacturing an optical component (100) according to claim 8, wherein the material removal during the polishing step that follows step f) is comprised between 1 and 20 microns. 10. The method of manufacturing an optical component (100) according to claim 1, including a method of hardening the optical component (100) with respect to power laser radiations, said hardening method comprising the steps of: h. Inspecting the polished or finished optical surface (110) of the optical component (100) to detect and locate at least one surface defect to be eliminated (120) on the optical surface (110) of the optical component (100);i. For each surface defect to be eliminated located at step h), applying a laser beam over an area encompassing the surface defect (120), said laser beam having a laser emission wavelength suitable for being absorbed by said material, so as to produce a local remelting of the fusible material, the power density of the laser beam and the duration of application of the laser beam being function of the transverse dimensions of the surface defect to be eliminated located at step h), so as to form, in place of the surface defect to be eliminated (120), an area of laser remelted material (310);j. Resuming the method of manufacturing the optical component at step c) of the method of claim 1 when step i) has been performed before the end of step c); or, respectively, at step d) when step i) has been performed after the end of step c). 11. The method of manufacturing an optical component (100) of claim 1, wherein said method comprises said steps a), b), and c): a. the step of roughing (10) the optical component (100) to form the at least one optical surface (110) on said substrate;b. the step of smooth grinding (20) said optical surface (110) of the optical component (100) so as to obtain the smoothed optical surface; andc. the step of polishing (40) said smoothed optical surface so as to obtain a polished optical surface,wherein said method further comprises, after at least one of the group consisting of said step b) and said step c), performing said steps e), f), and g):e. the step of inspecting (30′, 50′, 70′) the smoothed or polished optical surface of the optical component to detect and locate the at least one surface defect to be eliminated (120) on the smoothed or polished optical surface of the optical component;f. the step of, for each surface defect to be eliminated (120) located at said step e), applying the laser beam (35, 55, 75) over the area encompassing said surface defect to be eliminated, so as to produce the local remelting of the fusible material, so as to form, in place of the surface defect to be eliminated, the area of laser remelted material (310); andg. the step of continuing the method of manufacturing the optical component at said step c) when said step f) has been performed before the end of said step c). 12. The method of manufacturing an optical component (100) of claim 11, wherein said method further comprises said step d), the step of finishing (60) said polished optical surface so as to obtain the finished optical surface, andwherein said method further comprises, after at least one of the group consisting of said step b) and said step c), performing said steps e), f), and g):e. the step of inspecting (30′, 50′, 70′) the smoothed or polished optical surface of the optical component to detect and locate the at least one surface defect to be eliminated (120) on the smoothed or polished optical surface of the optical component;f. the step of, for each surface defect to be eliminated (120) located at said step e), applying the laser beam (35, 55, 75) over the area encompassing said surface defect to be eliminated, so as to produce the local remelting of the fusible material, so as to form, in place of the surface defect to be eliminated, the area of laser remelted material (310); andg. the step of i) continuing the method of manufacturing the optical component at step c) when said step f) has been performed before the end of said step c); or, respectively, ii) continuing the method of manufacturing the optical component at said step d) when said step f) has been performed after the end of said step c). 13. The method of manufacturing an optical component (100) of claim 12, wherein said step g. comprises the step of continuing the method of manufacturing the optical component at said step c) when said step f) has been performed before the end of said step c). 14. The method of manufacturing an optical component (100) of claim 12, wherein said step g. comprises the step of continuing the method of manufacturing the optical component at said step d) when said step f) has been performed after the end of said step c).
연구과제 타임라인
LOADING...
LOADING...
LOADING...
LOADING...
LOADING...
이 특허에 인용된 특허 (5)
McCluskey Douglas (Greenlane PA) Kelchner Harley E. (Hatfield PA), Apparatus for repair of shatterproof glass.
Lin, Yung-Yu, Inspecting device for detecting appearance of debris on a surface of a glass substrate, inspecting apparatus and method for conducting inspection.
Koike,Kesahiro; Miyagaki,Junji, Method of producing a glass substrate for a mask blank, method of producing a mask blank, and method of producing a transfer mask.
Heineken Alfred H. (Amsterdam NLX) Baumert Reinhard (Frankfurt DEX) Gaar Hans (Frankfurt DEX) Hoffmann Ulrich (Frankfurt DEX) Roth Ulrigh (Frankfurt DEX) Schwmmlein Wolfgang (Frankfurt DEX), Method of, and apparatus for, repairing mechanical and/or chemical damage to the surface of bottles destined for re-use.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.