NTIS 바로가기大韓機械學會論文集. Transactions of the Korean Society of Mechanical Engineers. A. A, v.24 no.3 = no.174, 2000년, pp.710 - 717
김정규 , 김철수 , 조동혁 , 김도식 , 윤인수
Tensile and fracture toughness tests of the cold-rolled STS 304 steel plate for membrane material of LNG storage tank were performed at wide range of temperatures, 11 IK(boiling point of LNG), 153K , 193K and 293K(room temperature). Tensile strength significantly increases with a decrease in tempera...
* AI 자동 식별 결과로 적합하지 않은 문장이 있을 수 있으니, 이용에 유의하시기 바랍니다.
한국가스공사 최종보고서, 1995, 'LNG저장탱크용 Membrane 개발 및 응력해석,' DD-CR-031-92049509
Reed, R. P. and Tobler, R. L., 1982, 'Deformation of Metastable Austenitic Steels at Low Temperatures,' Advances in Cryogenic Engineering - Materials, Vol. 28, pp. 49~56
Guntner, C. J. and Reed, R. P., 1962, 'The Effect of Experimental Variables Including the Martensitic Transformation on the Low-Temperature Mechanical Properties of Austenitic Stainless Steel,' Transactions of the ASM, Vol. 55, pp. 399-419
Tobler, R. L. and Reed, R. P., 1982, 'Tensile and Fracture Properties of Manganese-modified AISI 304 Type Stainless Steel,' Advances in Cryogenic Engineering - Materials, Vol. 28, pp. 83-92
Shimada, M., Tobler, R. L., Shoji, T. and Takahashi, H., 1989, ''Size, Side-Grooving, and Fatigue Precracking Effects on J - integral Test Results for SUS 304 Stainless Steel at 4K,' Advances in Cryogenic Engineering - Materials, Vol. 34, pp. 259-266
'Standard Test Method for Tension Testing of Metallic Materials,' 1993, Annual Book of ASTM Standards, E8M-97
'Standard Test Method for J - Integral Characterization of Fracture Toughness,' 1996, Annual Book of ASTM Standards, E1737-96.
Huang, G. L., Matlock, D. K. and Kauss, G., 1989, 'Martensite Formation, Strain Rate Sensitivity, and Deformation Behavior of Type 304 Stainless Steel Sheet,' Metallurgical Transactions A, Vol. 20A, No. 7, pp. 1239-1246
小寺澤 良一, 1981, 'フラクトグラフイイとその應用', 日刊工業新聞社, pp. 39-42
Suzuki, T., Kojima, H., Suzuki, K., Hasimoto, T., Koike, S. and Ichihara, T., 1976, 'Plastic Deformation and Martensitic Transformation in an Iron-base Alloy,' Scripta Metallurgica, Vol. 10, pp. 353-358
Paris, P. C, Tada, H., Zahoor, A. and Ernst, H., 1979, 'The Theory of Instability of the Tearing Mode for Elastic-plastic Crack Growth', ASTM STP 668, pp. 5-36
오세욱, 안광주, 윤영 재, 1986, 'SB강의 평활 및 측면홈 CT시험편의 $J_{IC}$ 평가,' 대한기계학회논문집, 제10권, 제4호, pp. 494-503
中村春夫, 小林英男, 中澤 一, 1979, 'ストレッチゾ-ン幅のJ-積分による評價彈とその彈塑性破壞じん性試驗への適用,' 日本機械學會 論文集, Vol. 45, No. 392, .pp. 336-345
Sreenivasan, P. R., Ray, S. K. Vaidyanathan, S. and Rodriguez, P. ,1996, 'Measurement of Stretch Zone Height and Its Relationship to Crack Tip Opening Displacement and Initiation J-value in an AISI 316 Stainless Steel', Fatigue & Fracture of Engineering Materials and Structures, Vol. 19, No. 7, pp. 855-868
Brothers, A. J., Hill, M., Parker, M. T., Spitzig, W. A., Wiebe, W. and Wolff, U. E., 1971, 'Correlation of Fracture Toughness, $K_{IC}$ , with Fractographically Derived Plastic Stretched Zone Width-A Report of ASTM E-24/II Task Group,' ASTM STP 493, pp. 3-19
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.