NTIS 바로가기Carbon, v.33 no.4, 1995년, pp.359 - 365
Yamamoto, O. (Department of Chemical Technology, Kanagawa Institute of Technology, 1030 Shimo-ogino, Atsugishi, 243-02 Japan) , Sasamoto, T. (Department of Chemical Technology, Kanagawa Institute of Technology, 1030 Shimo-ogino, Atsugishi, 243-02 Japan) , Inagaki, M. (Department of Applied Chemistry, Faculty of Engineering, Hokkaido University, Kita-ku, Sapporo, 060 Japan)
AbstractAfter the formation of a concentration gradient of SiC within a carbon-carbon composite, a zircon (ZrSiO4) thin film was coated on the surface. Oxidation-resistance tests of the treated CC composites were then carried out. A concentration gradient of SiC was produced by heating the C...
Konkin 1985 Strong Fibers
Adv. Comp. Klein 38 1989
Rogers 202 1973 New Horiz. Mater. Process., Nat. SAMPE Symp. Exhib. 18th
Carbon McKee 26 659 1988 10.1016/0008-6223(88)90068-1
Carbon McKee 24 737 1986 10.1016/0008-6223(86)90183-1
J. Am. Ceram. Soc. Filipuzzi 77 459 1994 10.1111/j.1151-2916.1994.tb07015.x
J. Mater. Sci. Ogawa 11 296 1992
J. Am. Ceram. Soc. Nixon 75 703 1992 10.1111/j.1151-2916.1992.tb07862.x
Seramikkusu-Gakujyutsu-Ronbun-Shi Kawai 99 390 1991 10.2109/jcersj.99.390
J. Eur. Ceram. Soc. Yamamoto 12 435 1993 10.1016/0955-2219(93)90076-4
Seramik-kusu-Gakujyutsu-Ronbun-Shi Yamamoto 102 165 1994 10.2109/jcersj.102.165
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.