NTIS 바로가기Journal of materials research, v.15 no.12, 2000년, pp.2857 - 2863
Lu, Guo-Quan , Calata, Jesus Noel
Cordierite glass-ceramic coatings do not bond to molybdenum directly because of the absence of a suitable transition layer. Dual metallic interlayers of copper/chromium and nickel/chromium were electroplated on the substrates to enhance adhesion. The adhesion of the glass-ceramic coatings was evalua...
The Materials Science of Thin Films 419 1992 Ohring
11. Private discussions by T. Kuhr with G.V. Gibbs on cordierite at V.P.I. & S.U. (Spring 1997).
9. Ceramic Films and Coatings, edited by J.B. Wachtman and R.A. Haber (Noyes Publications, Park Ridge, NJ, 1993), p. 289.
Marshall, D. B., Evans, A. G.. Measurement of adherence of residually stressed thin films by indentation. I. Mechanics of interface delamination. Journal of applied physics, vol.56, no.10, 2632-2638.
Rossington, C., Evans, A. G., Marshall, D. B., Khuri-Yakub, B. T.. Measurements of adherence of residually stressed thin films by indentation. II. Experiments with ZnO/Si. Journal of applied physics, vol.56, no.10, 2639-2644.
Surface Engineering 5 3 1994
Practical Electroplating Handbook 1989 Parthasaradhy
10. Materials Science and Engineering Handbook, 2nd ed., edited by J.F. Shackleford, W. Alexander, and J.S. Park (CRC Press, Boca Raton, FL, 1994).
Cao, H.C., Evans, A.G.. An experimental study of the fracture resistance of bimaterial interfaces. Mechanics of materials : an international journal, vol.7, no.4, 295-304.
Ashcroft, I. A., Derby, B.. Adhesion testing of glass-ceramic thick films on metal substrates. Journal of materials science, vol.28, no.11, 2989-2998.
1. Lu G-Q. , Calata J.N. , Bang J. , Kuhr T. , and Amith A. , Final Project Report to Triad Investors Corp. (1997).
8. Bang J. , Calata J. , and Lu G-Q. (unpublished).
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.