Legrand, L (Corresponding author. Fax: +33-1-69477655) , Savoye, S (Laboratoire Analyse et Environnement, UMR 8587, CNRS, Université) , Chausse, A (d'Evry Val d'Essonne, Bd F. Mitterand, UMR8587, 91025 Evry Cedex, France) , Messina, R (Laboratoire Analyse et Environnement, UMR 8587, CNRS, Université)
AbstractOxidation layers formed on iron in deaerated bicarbonate/carbonate solutions at potentials in the active range were investigated through electrochemical techniques, FTIR and scanning electron microscopy. Three oxidation products have been obtained, siderite, am-FeOOH with adsorbed carbonate ...
Corrosion NACE Davies 36 416 1980 10.5006/0010-9312-36.8.416
Corrosion Sci. Valentini 25 985 1985 10.1016/0010-938X(85)90067-8
Corrosion Sci. Castro 32 37 1991 10.1016/0010-938X(91)90062-T
Electrochim. Acta Castro 36 117 1991 10.1016/0013-4686(91)85188-D
J. Electroanal. Chem. Rubim 258 327 1989 10.1016/0022-0728(89)85118-6
Electrochim. Acta Odziemkowski 39 2225 1994 10.1016/0013-4686(94)E0171-U
Corrosion Sci. Odziemkowski 40 371 1998 10.1016/S0010-938X(97)00141-8
J. Electrochem. Soc. Simpson 143 2146 1996 10.1149/1.1836973
Corrosion Sci. Blengino 37 621 1995 10.1016/0010-938X(94)00160-8
Corrosion Sci. Drissi 37 2025 1995 10.1016/0010-938X(95)00096-3
Clay Miner. Taylor 15 369 1980 10.1180/claymin.1980.015.4.04
J. Mater. Sci. Markov 25 3096 1990 10.1007/BF00587656
Clays Clay Miner. Su 45 814 1997 10.1346/CCMN.1997.0450605
Corrosion NACE Heuer 54 566 1998 10.5006/1.3284885
Corrosion Sci. Drissi 37 2025 1995 10.1016/0010-938X(95)00096-3
Corrosion Sci. Refait 40 1547 1998 10.1016/S0010-938X(98)00066-3
해당 논문의 주제분야에서 활용도가 높은 상위 5개 콘텐츠를 보여줍니다.
더보기 버튼을 클릭하시면 더 많은 관련자료를 살펴볼 수 있습니다.
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.