NTIS 바로가기Cement & concrete composites, v.112, 2020년, pp.103680 -
Jun, Yubin (Department of Civil and Environmental Engineering, Korea Advanced Institute of Science and Technology) , Kim, Taewan (Department of Civil Engineering, Pusan National University) , Kim, Jae Hong (Department of Civil and Environmental Engineering, Korea Advanced Institute of Science and Technology)
Abstract This paper presents the microstructural properties of KOH-activated slag pastes produced with natural seawater under different salinity levels. The seawater-mixed samples exhibit higher 91-day strength compared to the control sample produced with deionized water. Their reduced total porosi...
Rain and Freshwater, World Meteorological Organization.https://public.wmo.int.
Concr. Int. Mehta 23 2002 Greening of the concrete industry for sustainable development
IES J. Part A Civ. Struct. Eng. Wegian 3 4 235 2010 10.1080/19373260.2010.521048 Effect of seawater for mixing and curing on structural concrete
Cement Concr. Compos. Kaushik 17 3 177 1995 10.1016/0958-9465(95)00015-5 Suitability of sea water for mixing structural concrete exposed to a marine environment
Concr. Int. Neville 23 1 48 2001 Seawater in the mixture
Nishida 2013 Third Int. Conf. Sustain. Constr. Mater. Technol., Kyoto, Japan Some considerations for the applicability of seawater as mixing water in concrete
Otsuki 2011 36th Conf. World Concr. Struct. Possibility of sea water as mixing water in concrete
Construct. Build. Mater. Wang 191 891 2018 10.1016/j.conbuildmat.2018.10.010 Multiscale investigations on hydration mechanisms in seawater OPC paste
Ceram. Int. El-Didamony 38 3773 2012 10.1016/j.ceramint.2012.01.024 Properties and durability of alkali-activated slag pastes immersed in sea water
Appl. Sci. Jun 7 10 2017 10.3390/app7100971 A comparison study for chloride-binding capacity between alkali-activated fly ash and slag in the use of seawater
Construct. Build. Mater. Richardson 168 404 2018 10.1016/j.conbuildmat.2018.02.034 Composition and structure of an 18-year-old 5M KOH-activated ground granulated blast-furnace slag paste
Cement Concr. Res. Jambunathan 54 143 2013 10.1016/j.cemconres.2013.09.009 The role of alumina on performance of alkali-activated slag paste exposed to 50°C
Cement Concr. Res. Wang 25 3 561 1995 10.1016/0008-8846(95)00045-E Hydration products of alkali activated slag cement
2014 Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency
2016 Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. Or [50-mm] Cube Specimens)
PDF-2 database. In: Data ICDD, editor. Newton Square, PA2000.
Acta Crystallogr. A Allmann 63 5 412 2007 10.1107/S0108767307038081 The introduction of structure types into the inorganic crystal structure database ICSD
2008 Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete
1997 Standard Test Method for Water-Soluble Chloride in Mortar and Concrete
Cement Concr. Res. Haha 41 9 955 2011 10.1016/j.cemconres.2011.05.002 Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag - Part I: effect of MgO
Barnes 2002 Structure and Performance of Cements
Cement Concr. Res. Schneider 31 7 993 2001 10.1016/S0008-8846(01)00530-0 29Si and 27Al high-resolution NMR characterization of calcium silicate hydrate phases in activated blast-furnace slag pastes
Thermochim. Acta Grishchenko 570 74 2013 10.1016/j.tca.2013.07.030 Thermodynamic properties and thermal behavior of Friedel's salt
Cement Concr. Compos. Kayali 34 8 936 2012 10.1016/j.cemconcomp.2012.04.009 The role of hydrotalcite in chloride binding and corrosion protection in concretes with ground granulated blast furnace slag
Appl. Clay Sci. Grover 48 4 631 2010 10.1016/j.clay.2010.03.017 Synthetic hydrotalcite-type and hydrocalumite-type layered double hydroxides for arsenate uptake
Chem. Mater. Bontchev 15 19 3669 2003 10.1021/cm034231r Synthesis, characterization, and ion exchange properties of hydrotalcite Mg6Al2(OH)16(A)x(A')2-x·4H2O (A, A' = Cl-, Br-, I-, and NO3-, 2 ≥ x ≥ 0) derivatives
Eng. Geol. Wild 51 1 37 1998 10.1016/S0013-7952(98)00039-8 Effects of partial substitution of lime with ground granulated blast furnace slag (GGBS) on the strength properties of lime-stabilised sulphate-bearing clay soils
Geosci. J. Moon 15 3 287 2011 10.1007/s12303-011-0023-y Impact of brownmillerite hydration on Cr(VI) sequestration in chromite ore processing residue
Mater. Corros. Yang 64 12 1066 2013 10.1002/maco.201206915 Modified hydrotalcites as a new emerging class of smart additive of reinforced concrete for anticorrosion applications: a literature review
J. Adv. Concr. Technol. Hirao 3 1 77 2005 10.3151/jact.3.77 Chloride binding of cement estimated by binding isotherms of hydrates
Cement Concr. Res. Lambert 15 4 675 1985 10.1016/0008-8846(85)90068-7 Pore solution chemistry of the hydrated system tricalcium silicate/sodium chloride/water
Cement Concr. Res. Kim 54 208 2013 10.1016/j.cemconres.2013.09.011 Use of CaO as an activator for producing a price-competitive non-cement structural binder using ground granulated blast furnace slag
J. Hazard Mater. Islam 169 1 524 2009 10.1016/j.jhazmat.2009.03.128 Nitrate sorption by thermally activated Mg/Al chloride hydrotalcite-like compound
Cement Concr. Res. Ben Haha 41 3 301 2011 10.1016/j.cemconres.2010.11.016 Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags
Cement Concr. Res. Payá 33 4 603 2003 10.1016/S0008-8846(02)01026-8 Evaluation of the pozzolanic activity of fluid catalytic cracking catalyst residue (FC3R). Thermogravimetric analysis studies on FC3R-Portland cement pastes
J. Ind. Eng. Chem. Palmer 17 1 56 2011 10.1016/j.jiec.2010.10.009 The effect of high concentrations of calcium hydroxide in neutralised synthetic supernatant liquor-implications for alumina refinery residues
J. Mater. Chem. Kuwahara 20 24 5052 2010 10.1039/c0jm00518e A novel conversion process for waste slag: synthesis of a hydrotalcite-like compound and zeolite from blast furnace slag and evaluation of adsorption capacities
Thermochim. Acta Kristóf-Makó 342 1 105 1999 10.1016/S0040-6031(99)00290-7 The effect of mechanical treatment on the crystal structure and thermal decomposition of dolomite
Thermochim. Acta McCauley 185 2 271 1991 10.1016/0040-6031(91)80049-O Decrepitation and thermal decomposition of dolomite
L. Reh, L. Plass, H.W. Schmidt, G. Schoene, P. Marchessaux, Process for Thermal Decomposition of Aluminum Chloride Hexahydrate, Patent US4080437A (1978).
Heron Nijland 46 4 253 2001 Unraveling the temperature distribution in fire-damaged concrete by means of PFM microscopy: outline of the approach and review of potentially useful reactions
해당 논문의 주제분야에서 활용도가 높은 상위 5개 콘텐츠를 보여줍니다.
더보기 버튼을 클릭하시면 더 많은 관련자료를 살펴볼 수 있습니다.
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.