NTIS 바로가기Engineering fracture mechanics, v.31 no.2, 1988년, pp.339 - 347
Hoshide, T. , Ohara, T. , Yamada, T.
Most of the previous investigations on fatigue of ceramic materials have been conducted experimentally as well as theoretically under constant stress amplitude conditions. However, both a theoretical approach and experimental data for variable stress amplitude loadings will be necessary to improve t...
Int. J. Fracture Evans 16 485 1980 10.1007/BF02265214 Fatigue in ceramics
Int. J. Fracture Aoki 21 285 1983 10.1007/BF00942347 Statistical approach to time-dependent failure of brittle material
Yamada 2 441 1985 Reliability of ceramic materials for static and cyclic loads
Prog. Mater. Sci. Evans 21 191 1976 10.1016/0079-6425(76)90006-2 Structural ceramics
Int. J. Fracture Hoshide 26 229 1984 10.1007/BF01140630 Fracture mechanics approach to evaluation of strength in sintered silicon nitride
Engng Fracture Mech. Usami 23 745 1986 10.1016/0013-7944(86)90120-7 Strength of ceramic materials containing small flaws
Yamada 31 51 1986 Behavior of cyclic fatigue strength and inherent flaws of ceramics
Hertzberg 562 1983 Deformation and Fracture Mechanics of Engineering Materials
T. Hoshide, T. Ohara and T. Yamada, Fatigue crack growth from indentation flaw in ceramics. Int. J. Fracture (in press).