NTIS 바로가기Journal of laser applications, v.22 no.3, 2010년, pp.116 - 119
Choi, Kwang-Deok (Advanced Welding & Joining Technology Research Team, Korea Institute of Industrial Technology, 7-47 Songdo-Dong, Yeonsu-Gu, Incheon 406-840, Korea) , Ahn, Young-Nam (Advanced Welding & Joining Technology Research Team, Korea Institute of Industrial Technology, 7-47 Songdo-Dong, Yeonsu-Gu, Incheon 406-840, Korea) , Kim, Cheolhee (Advanced Welding & Joining Technology Research Team, Korea Institute of Industrial Technology, 7-47 Songdo-Dong, Yeonsu-Gu, Incheon 406-840, Korea)
Laser welding of aluminum alloys usually produces linear welds that have shear-tensile strength lower than that of the base metal. This is usually due to porosity resulting from an unstable keyhole and cracking which is related to the high crack sensitivity of many of these alloys. In this work lase...
Kobelco Technol. Rev. 26 55 2005 Wrought aluminum technologies for automobiles
Int. Mater. Rev. 44-6 238 1999 10.1179/095066099101528298 Current issues and problems in laser welding of automotive aluminium alloys
Weld. Int. 17-3 173 2003 10.1533/wint.2003.3074 Recent Technological development in welding of aluminium and its alloys
Sci. Technol. Weld. Join. 6-3 182 2001 10.1179/136217101101538730 CO2 and Nd-YAG laser beam welding of 5754-O aluminium alloy for automotive applications
J. Mater. Process. Technol. 115-1 2 2001 10.1016/S0924-0136(01)00756-7 Light-weight structures produced by laser beam joining for future applications in automobile and aerospace industry
Metall. Trans. A 16A-7 1345 1985 Grain structure and solidification cracking in oscillated arc welds of 5052 aluminum alloy
Sci. Technol. Weld. Joining 14-2 161 2009 10.1179/136217108X386554 Characterisation of solidification cracking in pulsed Nd:YAG laser welding of 2024 aluminium alloy
Weld. J. 45-6 241s 1966 Preventing weld cracks in high strength aluminium alloys
J. Inst. Met. 74 439 1948 Cracking during the casting and welding of the more common binary aluminium alloys
Weld. J. 31-10 448s 1952 Weld cracking of aluminum alloys
Int. J. KWS 1-1 63 2001 Effect of the Mg content on the solidification cracking susceptibility of the Al-Mg alloy laser welds
Int. J. KWS 2-2 42 2002 Solidification cracking susceptibility of Al-Mg-Si Alloy Laser Welds
Weld. World 50-11/12 46 2006 Influence of the weld metal chemical composition on the solidification cracking susceptibility of AA6056-T4 alloy
Weld. J. 87-1 18s 2008 Effects of Temporal Pulse Shaping on Cracking Susceptibility of 6061-T6 Aluminum Nd:YAG Laser Welds
277 2008
Mater. Sci. Eng., A 519-1-2 167 2009 The relation between liquation and solidification cracks in pulsed laser welding of 2024 aluminium alloy
180 1998
2008
27 2009
Trans. JWRI 11-2 87 1982 A new test specimen for self-restraint solidification crack susceptibility test of electron-beam welding bead
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.