NTIS 바로가기Electrochimica acta, v.278, 2018년, pp.176 - 181
Okubo, Keisuke (Department of Applied Chemistry, Graduate School of Engineering, Kyushu University) , Wang, He (Department of Applied Chemistry, Graduate School of Engineering, Kyushu University) , Hayashi, Katsuro (Department of Applied Chemistry, Graduate School of Engineering, Kyushu University) , Inada, Miki (Department of Applied Chemistry, Graduate School of Engineering, Kyushu University) , Enomoto, Naoya (Department of Applied Chemistry, Graduate School of Engineering, Kyushu University) , Hasegawa, George (Department of Applied Chemistry, Graduate School of Engineering, Kyushu University) , Osawa, Takashi (Department of Materials Science, Graduate School of Engineering, Tohoku University) , Takamura, Hitoshi (Department of Materials Science, Graduate School of Engineering, Tohoku University)
Abstract Ceramic sheet of Na+ ion-conducting solid electrolyte, Na3Zr2Si2PO12 (NASICON), has been prepared by tape-casting method. Addition of 60Na2O-10Nb2O5-30P2O5 glass as a sintering aid is crucial for fabrication of fully-densified impermeable sheet. Otherwise the gas tightness is not achieved ...
J. Electrochem. Soc. Goodenough 162 A2387 2015 10.1149/2.0021514jes Review-solid electrolytes in rechargeable electrochemical cells
Nat. Energy Janek 1 16141 2016 10.1038/nenergy.2016.141 A solid future for battery development
J. Appl. Glass Sci. Tatsumisago 5 226 2014 10.1111/ijag.12084 Sulfide glass-ceramic electrolytes for all-solid-state lithium and sodium batteries
S. J. Visco, Y. S. Nimon, Active metal/aqueous electrochemical cells and systems, US Patent 2004/0197641.
J. Am. Chem. Soc. Ding 135 4450 2013 10.1021/ja312241y Dendrite-free lithium deposition via self-healing electrostatic shield mechanism
Nat. Nanotechnol. Zheng 9 618 2014 10.1038/nnano.2014.152 Polymer nanofiber-guided uniform lithium deposition for battery electrodes
Nanomater. Energy Sun 2 801 2013 10.1016/j.nanoen.2013.02.003 Lithium ion conducting membranes for lithium-air batteries
J. Solid State Electrochem. Visco 18 1443 2014 Aqueous and nonaqueous lithium-air batteries enabled by water-stable lithium metal electrodes
J. Electrochem. Soc. Takahashi 159 A1065 2012 10.1149/2.072207jes A Water stable high lithium ion conducting Li1.4Ti1.6Al0.4(PO4)3-epoxy resin hybrid sheet
J. Electrochem. Soc. Zhang 162 A1265 2015 10.1149/2.0711507jes Tape-cast water-stable NASICON-type high lithium ion conducting solid electrolyte films for aqueous lithium-air batteries
Langmuir Lancel 33 9288 2017 10.1021/acs.langmuir.7b00675 Hybrid Li-ion conducting membrane as protection of Li-anode in aqueous Li-air battery: coupling sol-gel chemistry and electrospinning
Solid State Ionics Safanama 262 211 2014 10.1016/j.ssi.2013.11.031 Lithium conducting solid electrolyte Li1+xAlxGe2−x(PO4)3 membrane for aqueous lithium air battery
J. Electrochem. Soc. Jiménez 163 A1653 2016 10.1149/2.0881608jes Lithium La0. 57Li0. 33TiO3 Perovskite and Li1.3Al0.3Ti1.7 (PO4)3 Li-NASICON supported thick films electrolytes prepared by tape casting method
Chem. Rev. Yabuuchi 114 11636 2014 10.1021/cr500192f Research development on sodium-ion batteries
Curr. Opin. Solid State Mater. Sci. Ellis 16 168 2012 10.1016/j.cossms.2012.04.002 Sodium and sodium-ion energy storage batteries
Nat. Chem. Larcher 7 19 2015 10.1038/nchem.2085 Towards greener and more sustainable batteries for electrical energy storage
Solid State Ionics Auborn 5 315 1981 10.1016/0167-2738(81)90256-3 Conductivity of NASICON ceramic membranes in aqueous solution
J. Electrochem. Soc. Hayashi 160 A1467 2013 10.1149/2.067309jes A mixed aqueous/aprotic sodium/air cell using a NASICON ceramic separator
J. Electrochem. Soc. Liang 162 A1215 2015 10.1149/2.0421507jes A high-energy-density mixed-aprotic-aqueous sodium-air cell with a ceramic separator and a porous carbon electrode
Electrochim. Acta Hashimoto 182 809 2015 10.1016/j.electacta.2015.09.153 Aqueous and nonaqueous sodium-air cells with nanoporous gold cathode
Solid State Ionics von Alpen 3/4 215 1981 10.1016/0167-2738(81)90085-0 Compositional dependence of the electrochemical and structural parameters in the NASICON system (Na1+xSixZr2P3−xO12)
Electrochim. Acta Noguchi 101 59 2013 10.1016/j.electacta.2012.11.038 Fabrication and performances of all solid-state symmetric sodium battery based on NASICON-related compounds
J. Power Sources Lalère 247 975 2014 10.1016/j.jpowsour.2013.09.051 An all-solid state NASICON sodium battery operating at 200 °C
ACS Cent. Sci. Zhou 3 52 2017 10.1021/acscentsci.6b00321 Rechargeable sodium all-solid-state battery
Angew. Chem. Gao 129 5633 2017 10.1002/ange.201702003 A plastic-crystal electrolyte interphase for all-solid-state batteries
Solid State Ionics Shimizu 132 143 2000 10.1016/S0167-2738(00)00703-7 Sol-gel processing of NASICON thin film using aqueous complex precursor
J. Am. Ceram. Soc. Noi 101 1255 2018 10.1111/jace.15288 Liquid-phase sintering of highly Na+ ion conducting Na3Zr2Si2PO12 ceramics using Na3BO3 additive
Scr. Mater. Suzuki 145 67 2018 10.1016/j.scriptamat.2017.10.010 Low temperature sintering of Na1+xZr2SixP1−xO12 by addition of Na3BO3
Solid State Ionics Wang 2018 Low temperature-densified NASICON-based ceramics promoted by Na2O-Nb2O5-P2O5 glass additive and spark plasma sintering
Solid State Ionics Honma 269 19 2015 10.1016/j.ssi.2014.11.009 Electrical conductivity of Na2O-Nb2O5-P2O5 glass and fabrication of glass-ceramic composites with NASICON type Na3Zr2Si2PO12
J. Membr. Sci. Hayamizu 462 147 2014 10.1016/j.memsci.2014.03.038 Effects of surface modification on the oxygen permeation of Ba0.5Sr0.5Co0.8Fe0.2O3−δ membrane
Solid State Ionics Gordon 3/4 243 1981 10.1016/0167-2738(81)90091-6 Fabrication and characterization of Nasicon electrolytes
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.