초록
▼
An improved process for forming a non-woven fabric by wet-laying, on paper making equipment, staple length, synthetic fibers having a length to diameter ratio of about 400 to 3000, and an improved, non-woven fabric produced by the process. The process involves forming a stable, viscous, uniform, air
An improved process for forming a non-woven fabric by wet-laying, on paper making equipment, staple length, synthetic fibers having a length to diameter ratio of about 400 to 3000, and an improved, non-woven fabric produced by the process. The process involves forming a stable, viscous, uniform, air-fiber-water dispersion by: adding the fibers to a high-shear agitated mixture of water and a dispersant to separate the fibers and to completely and uniformly distribute the individual fibers throughout the resulting, high-shear agitated, air, water and fiber mixture; and then, slowly adding a thixotropic thickener to the high-shear agitated mixture to form the viscous, air-fiber-water dispersion, having a nascent viscosity of about 10 to 125 cps., when measured at a shear rate of 30.5 sec.-1, and in which the individual fibers are restrained from becoming entangled and from forming knits, bundles, and strings.
대표청구항
▼
In a process for diluting a stable, viscous, uniform, air, fiber and water dispersion, which contains about 1% to 10% by volume of entrained air and about 0.03% to 1.0% by weight of staple length fibers, at least about 10% by weight of the fibers having a length to diameter ratio of about 400 to 300
In a process for diluting a stable, viscous, uniform, air, fiber and water dispersion, which contains about 1% to 10% by volume of entrained air and about 0.03% to 1.0% by weight of staple length fibers, at least about 10% by weight of the fibers having a length to diameter ratio of about 400 to 3000, and which has a nascent viscosity of about 10 to 125 cps., when measured at a shear rate of 30.5 sec.-1; with a viscous aqueous diluting medium, which contains about 1% to 10% by volume of entrained air and which has a nascent viscosity of about 5 to 30 cps., when measured at shear rate of 30.5 sec.-1; the improvement which comprises: feeding about one volume of the air, fiber, and water dispersion to the annulus ring of an eductor and feeding about two to twelve volumes of the diluting medium to the center feed of the eductor, just upstream of the vena contracta thereof, whereby the air, fiber and water dispersion is uniformly mixed with and distributed throughout the diluting medium, without undue entangling of the fibers.