IPC분류정보
국가/구분 |
United States(US) Patent
등록
|
국제특허분류(IPC7판) |
|
출원번호 |
US-0266787
(1994-06-28)
|
우선권정보 |
DK-0006956 (1988-12-14) |
국제출원번호 |
PCT/DK89/00295
(1989-12-14)
|
§371/§102 date |
19910624
(19910624)
|
국제공개번호 |
WO-9006902
(1990-06-28)
|
발명자
/ 주소 |
- Hansen Anders S. (Oksbol DKX) Davies Derek (Ashbourne GB2)
|
출원인 / 주소 |
- Danaklon A/S (Varde DKX 03)
|
인용정보 |
피인용 횟수 :
56 인용 특허 :
0 |
초록
▼
A method for producing a cement material with reduced development of self-induced cracking, the method comprising: adding to a concrete, mortar or cement mix to which water has been added, an amount of 0.05 to 1% by weight, based on the cementitious materials, of synthetic fiber bundles comprising 1
A method for producing a cement material with reduced development of self-induced cracking, the method comprising: adding to a concrete, mortar or cement mix to which water has been added, an amount of 0.05 to 1% by weight, based on the cementitious materials, of synthetic fiber bundles comprising 10-10,000 filaments per bundle, the filaments consisting essentially of a polyolefin, polyolefin derivative, a polyester or a mixture of the foregoing and having a length of 1-30 mm, a mean transverse dimension of 5-30 um and an aspect ratio of 100 to 1000, the filaments in each bundle being held together by a wetting agent, the wetting agent proving the individual filaments with a surface tension which allows them to become homogeneously dispersed in a concrete, mortar or paste mix with conventional mixing in conventional concrete mixing equipment, mixing the resultant mix for a period of at least 20 seconds to obtain a concrete, mortar or cement mix in which the individual filaments are homogeneously dispersed, and casting the concrete, mortar or paste mix in a configuration.
대표청구항
▼
A method for producing a cement material with reduced development of self-induced cracking, the method comprising: adding to a concrete, mortar or cement mix to which water has been added, an amount of 0.05 to 1% by weight, based on the cementitious materials, of synthetic fibre bundles comprising 1
A method for producing a cement material with reduced development of self-induced cracking, the method comprising: adding to a concrete, mortar or cement mix to which water has been added, an amount of 0.05 to 1% by weight, based on the cementitious materials, of synthetic fibre bundles comprising 10-10,000 filaments per bundle, the filaments consisting essentially of a polyolefin, a polyolefin derivative, a polyester or a mixture of the foregoing and having a length of 1 to 30 mm, a mean transverse dimension of 5 to 30 m100 to 1000, the filaments in each bundle being held together by a wetting agent, the wetting agent providing the individual filaments with a surface tension which allows them to become homogeneously dispersed in a concrete, mortar or paste with conventional mixing in conventional concrete mixing equipment, mixing the resulting mix for a period of at least about 20 seconds to obtain a concrete, mortar or paste mix in which the individual filaments are homogeneously distributed, and casting the concrete, mortar or paste mix in a configuration.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.