A method for repairing an article made of a fiber-reinforced ceramic matrix composite comprises attaching sections of a fiber-reinforced tape to the damaged area and then infiltrating the sections with the ceramic matrix or ceramic matrix precursor material. The material around the damaged area may
A method for repairing an article made of a fiber-reinforced ceramic matrix composite comprises attaching sections of a fiber-reinforced tape to the damaged area and then infiltrating the sections with the ceramic matrix or ceramic matrix precursor material. The material around the damaged area may be removed first to form a depression that is then filled with sections of the fiber-reinforced tape and further infiltrated with the ceramic matrix or ceramic matrix precursor material. The repaired article shows stress-strain curve similar to a defect-free article.
대표청구항
▼
1. A method for repairing a damaged area of an article that comprises a fiber-reinforced ceramic matrix composite (“CMC”) material, said method comprising:providing a repairing tape that comprises ceramic fibers and at least one matrix material selected from the group consisting of a c
1. A method for repairing a damaged area of an article that comprises a fiber-reinforced ceramic matrix composite (“CMC”) material, said method comprising:providing a repairing tape that comprises ceramic fibers and at least one matrix material selected from the group consisting of a ceramic matrix material, a ceramic matrix precursor material, and mixtures thereof;attaching at least a portion of said repairing tape to said damaged area of said article;providing an infiltrant phase material to said at least a portion of said repairing tape; said infiltrant phase material comprising a material selected from the group consisting of a ceramic matrix material, a ceramic matrix precursor material, and mixtures thereof; andinfiltrating said at least a portion of said repairing tape with said infiltrant phase material. 2. The method for repairing a damaged area of an article according to claim 1, wherein said repairing tape is prepared by placing said ceramic fibers next to each other to form a sheet having at least one layer of fibers, and at least a portion of one matrix material is disposed among said fibers. 3. The method for repairing a damaged area of an article according to claim 1, wherein said repairing tape comprises continuous fibers which are arranged substantially in parallel to one another and on which at least a portion of said matrix material is adhered. 4. The method for repairing a damaged area of an article according to claim 3, wherein said repairing tape is formed by winding on a support said continuous fibers on which said at least a portion of said matrix material is adhered. 5. The method for repairing a damaged area of an article according to claim 1, wherein said repairing tape is prepared by casting a mixture that comprises sections of said ceramic fibers and said at least one matrix material into a tape. 6. The method for repairing a damaged area of an article according to claim 1 further comprising cleaning said damaged area before attaching said at least a portion of said prepreg tape to said damaged area. 7. The method for repairing a damaged area of an article according to claim 1 further comprising removing a portion of said CMC material from said damaged area to form a depression in said article before attaching said at least a portion of said repairing tape to said damaged area, wherein said attaching comprises filling said depression with a plurality of layers of said repairing tape. 8. The method for repairing a damaged area of an article according to claim 7, wherein said depression has a shape selected from the group consisting of an inverted cone, an inverted truncated cone, and a prism. 9. The method for repairing a damaged area of an article according to claim 1, wherein said ceramic fibers comprise silicon carbide. 10. The method for repairing a damaged area of an article according to claim 9, wherein said ceramic fibers comprise silicon carbide and a coating comprising a nitride compound disposed on said fibers. 11. The method for repairing a damaged area of an article according to claim 10, wherein said nitride compound is selected from the group consisting of boron nitride, silicon nitride, silicon-doped boron nitride, and mixtures thereof. 12. The method for repairing a damaged area of an article according to claim 11, wherein said fibers comprise a plurality of coatings, each of said coatings comprising a different nitride compound. 13. The method for repairing a damaged area of an article according to claim 10, wherein said coating of said ceramic fibers has a graded composition across a thickness thereof. 14. The method for repairing a damaged area of an article according to claim 10, wherein said ceramic fibers further comprise at least another coating comprising a material selected from the group consisting of carbon, metal silicides, metal carbides, and metal borides. 15. The method for repairing a damaged area of an article according to claim 1, wherein said matrix material comprises a material selected from silicon and silicon carbide. 16. The method for repairing a damaged area of an article according to claim 1, wherein said infiltrant phase material is selected from the group consisting of silicon and silicon carbide. 17. The method for repairing a damaged area of an article according to claim 1, wherein said infiltrating is carried out by a melt infiltration. 18. The method for repairing a damaged area of an article according to claim 17, wherein said infiltrant phase material is silicon. 19. The method for repairing a damaged area of an article according to claim 17, wherein said infiltrating is carried out at a temperature up to and including an infiltration temperature used in an original manufacture of said article. 20. The method for repairing a damaged area of an article according to claim 17, wherein said infiltrating is carried out at a temperature from about 15° C. to about 20° C. less than an infiltration temperature used in an original manufacture of said article. 21. The method for repairing a damaged area of an article according to claim 20, wherein said infiltrating is carried out under an atmosphere of an inert gas. 22. The method for repairing a damaged area of an article according to claim 21, wherein said inert gas is selected from the group consisting of argon, helium, and mixtures thereof. 23. The method for repairing a damaged area of an article according to claim 19, wherein said infiltrating is carried out in a vacuum. 24. The method for repairing a damaged area of an article according to claim 23, wherein said vacuum is in a range from about 1 Pa to about 300 Pa. 25. The method for repairing a damaged area of an article according to claim 23, wherein said vacuum is from about 2 Pa to about 150 Pa. 26. The method for repairing a damaged area of an article according to claim 1, wherein said infiltrating is carried out by a chemical vapor deposition of said infiltrant phase material. 27. The method for repairing a damaged area of an article according to claim 1, wherein said infiltrating comprises infiltrating a melt of a precursor of said infiltrant phase material followed by pyrolyzing said precursor to form said infiltrant phase. 28. The method for repairing a damaged area of an article according to claim 1, wherein said infiltrant phase material comprises silicon and carbon. 29. The method for repairing a damaged area of an article according to claim 1, wherein said article is selected from the group consisting of combustion chamber liners, combinations of combustion liners and transition pieces, nozzles, shroud rings, vanes, buckets, and blades. 30. A method for repairing a damaged area of an article that comprises a fiber-reinforced CMC material, said method comprising:providing a repairing tape that comprises ceramic fibers and at least one matrix material selected from the group consisting of a ceramic matrix material, a ceramic matrix precursor material, and mixtures thereof;removing a portion of said CMC material from said damaged area to form a depression in said article, said depression having a shape selected from the group consisting of an inverted cone, an inverted truncated cone, and a prism having a base on a surface of said article;filling said depression with a plurality of portions of said repairing tape;providing an infiltrant phase material to said portions of said repairing tape;said infiltrant phase material comprising at least a material selected from the group consisting of a ceramic matrix material, a ceramic matrix precursor material, and mixtures thereof; andinfiltrating said portions of said repairing tape with said infiltrant phase material. 31. A method for repairing a damaged area of an article that comprises a fiber-reinforced CMC material, said method comprising:providing a repairing tape that comprises ceramic fibers and at least one matrix material selected from the group consisting of a ceramic matrix material, a c eramic matrix precursor material, and mixtures thereof;cleaning a portion of a surface of said article around said damaged area to provide a cleaned surface;attaching at least a portion of said repairing tape to said cleaned surface;providing an infiltrant phase material to said at least a portion of said repairing tape; said infiltrant phase material comprising at least a material selected from the group consisting of a ceramic matrix material, a ceramic matrix precursor material, and mixtures thereof; andinfiltrating said at least a portion of said repairing tape with said infiltrant phase material. 32. The method for repairing a damaged area of an article according to claim 31, said method further comprising attaching portions of said repairing tape to a wall of said depression before filling said depression with a plurality of portions of said repairing tape; wherein said ceramic fibers are silicon carbide fibers, and said matrix material and said infiltrant phase material comprise silicon and carbon. 33. The method for repairing a damaged area of an article according to claim 31, said method further comprising applying a layer of a material selected from ceramic matrix material, ceramic matrix precursor material, and mixtures thereof to a wall of said depression before filling said depression with a plurality of portions of said repairing tape. 34. The method for repairing a damaged area of an article according to claim 31, wherein said cleaning is carried out by heating said article in a reducing atmosphere. 35. The method for repairing a damaged area of an article according to claim 34, wherein said reducing atmosphere comprises a gas selected from the group consisting of hydrogen, carbon monoxide, and mixtures thereof with an inert gas. 36. The method for repairing a damaged area of an article according to claim 31, said method further comprising painting walls of said depression with a mixture comprising sections of said ceramic fibers and said at least one matrix material.