초록
▼
A method and apparatus for MIG welding is disclosed. When in an ac mode the output is unbalanced, or the balance may be controlled. The balance may be controlled to provide a desired deposition rate and/or to obtain a desired dilution. The frequency may be any frequency, for example 30 Hz, 60 Hz, 9
A method and apparatus for MIG welding is disclosed. When in an ac mode the output is unbalanced, or the balance may be controlled. The balance may be controlled to provide a desired deposition rate and/or to obtain a desired dilution. The frequency may be any frequency, for example 30 Hz, 60 Hz, 90 Hz, or more. The weld path may have groove with angle of less than 50 degrees. A consumable, cored, wire may be used, and provide at rates of 30 or 35 pounds per hour using a single arc. In various embodiments the balance may have a negative portion of at least 1. 5 times the positive portion. The process may be started using an extended negative portion, for example 0.5 or 0.75 seconds.
대표청구항
▼
The invention claimed is: 1. A method of MIG welding comprising: providing ac power to a weld, wherein the ac power has a negative portion and a positive portion, and the ac power further has a frequency; wherein the negative portion is greater than the positive portion; wherein the frequency is at
The invention claimed is: 1. A method of MIG welding comprising: providing ac power to a weld, wherein the ac power has a negative portion and a positive portion, and the ac power further has a frequency; wherein the negative portion is greater than the positive portion; wherein the frequency is at least 60 Hz; and providing a consumable, metal-cored, wire to the weld the wire includes providing a wire wherein the wire comprises a sheath encapsulating a core having a core composition, the core composition comprising a combination of graphite and one or more compounds of potassium, the combination of graphite and compounds of potassium in the core composition not exceeding approximately 5% by weight. 2. The method of claim 1, wherein the frequency is between 90 Hz and 120 Hz. 3. The method of claim 1, wherein providing the wire includes providing the wire electrode wherein the one or more compounds of potassium comprise K2MnTiO4. 4. The method of claim 3, wherein providing includes providing the wire wherein the combination is selected from the range from about 0.3% to about 5.0% by weight. 5. The method of claim 1, further comprising providing a weld path on at least one workpiece, wherein the weld path includes a groove having an angle of less than 30 degrees. 6. The method of claim 1, further comprising providing a weld path on at least one workpiece, wherein the weld path includes a groove having an angle of between 20 degrees and 30 degrees. 7. The method of claim 6 wherein the negative portion is at least 1.5 times the positive portion. 8. The method of claim 7 wherein the weld process begins with a first negative portion having a duration of at least 0.75 seconds. 9. The method of claim 1, including welding at a rate of at least 35 pounds per hour using a single arc. 10. The method of claim 9 including welding at a rate of at least 40 pounds per hour. 11. The method of claim 9 wherein the negative portion is at least twice the positive portion. 12. The method of claim 1 wherein the weld process begins with a first negative portion having a duration of at least 0.5 seconds. 13. The method of claim 1 further including providing a stick-out of about 2 inches. 14. The method of claim 13 further comprising providing a shielding gas at a rate of at least 80 cubic feet per hour. 15. The method of claim 1, further comprising providing a weld path on at least one workpiece, wherein the weld path includes a groove having an angle of less than 50 degrees. 16. A MIG welding system comprising: power means for providing ac power to a weld, wherein the ac power has a negative portion and a positive portion, and the ac power further has a frequency; and control means for controlling the power means, wherein the negative portion has a negative amp-seconds and the positive portion has a positive amp-seconds, wherein the control means causes the negative amp-seconds to be greater than the positive amp-seconds, and wherein the frequency is at least 60 Hz, and wherein the weld process begins with the negative portion of at least 0.5 seconds duration; and a source of wire comprising a sheath encapsulating a core having a core composition, the core composition comprising a combination of graphite and one or more compounds of potassium, the combination of graphite and compounds of potassium in the core composition not exceeding approximately 5% by weight. 17. The system of claim 16, wherein the control means includes means for providing the frequency to be between 90 Hz and 120 Hz. 18. The system of claim 16, further including a consumable, flux-cored, wire, disposed to be provided to the weld. 19. The system of claim 18, wherein the wire is metal-cored. 20. The system of claim 19, further comprising a weld path on at least one work piece, wherein the weld path includes a groove having an angle of less than 50 degrees. 21. The system of claim 16, further comprising a weld path on at least one workpiece, wherein the weld path includes a groove having an angle of less than 30 degrees. 22. The system of claim 21 wherein the control means for includes means for causing the negative amp-seconds to be at least twice the positive amp-seconds. 23. The system of claim 16 wherein the control means includes means for causing the negative amp-seconds to be at least 1.5 times the positive amp-seconds. 24. The system of claim 16 wherein the control means includes means for causing the weld process to begin with a first cycle portion having a duration of at least 0.75 seconds. 25. A method of controlling dilution in MIG welding comprising: providing ac power to a weld, wherein the ac power has a negative portion and a positive portion, and the ac power further has a frequency; controlling the balance of the negative portion and the positive portion to obtain a desired dilution. 26. The method of claim 25 wherein the negative portion is greater than the positive portion. 27. The method of claim 25 wherein the negative portion is less than the positive portion.