초록
▼
A sealing system, sealing system components, and methods of manufacture and use for a vessel that holds corrosive liquid, with the sealing system having a port on the vessel, an insert, and a sealing element. The sealing element is corrosion-resistant, essentially impermeable to corrosive and critic
A sealing system, sealing system components, and methods of manufacture and use for a vessel that holds corrosive liquid, with the sealing system having a port on the vessel, an insert, and a sealing element. The sealing element is corrosion-resistant, essentially impermeable to corrosive and critical fluids, essentially free of leachable impurities and is made with a material having a Shore A hardness between about 70 and about 95. A preferred material for the sealing ring is the class of materials known as polyolefins. The insert is operably engageable with the port and the sealing element to create a seal between the sealing element and the first and second sealing surfaces to prevent fluid flow through the port.
대표청구항
▼
It is claimed: 1. A system for holding critical fluids, the system comprising: a vessel that is made with polyethylene, has at least about 30 gallons of capacity, and a fluid contained therein, the fluid being a member of the group consisting of sulfuric acid, hydrochloric acid, hydrofluoric acid,
It is claimed: 1. A system for holding critical fluids, the system comprising: a vessel that is made with polyethylene, has at least about 30 gallons of capacity, and a fluid contained therein, the fluid being a member of the group consisting of sulfuric acid, hydrochloric acid, hydrofluoric acid, tetramethyl ammonium hydroxide, ammonium hydroxide, hydrogen peroxide, phosphoric acid, n-methyl pyridine, isopropyl alcohol, mixtures thereof, and mixtures thereof with other fluids; a port on the vessel; an insert mechanically engageable with the port; and a resilient non-fluoropolymer sealing element comprising a copolymer of ethylene and octene that is corrosion-resistant, essentially impermeable to the contents of the vessel, comprises a material having a Shore A hardness between about 75 and about 95, has less than 1000 ppm total trace metals as measured by digestion in nitric acid and has an exterior that seals against a first sealing surface on the port and against a second sealing surface on the insert; wherein the port, the insert, and the sealing element cooperate to form a seal between the sealing element and the first and second sealing surfaces that is adapted to hold at least 3 psi of air for at least 5 minutes. 2. The system of claim 1 wherein the sealing element material consists essentially of a single material having a Shore A hardness between about 75 and about 95. 3. The system of claim 2 wherein the sealing element consists essentially of a single continuous piece of the sealing element material. 4. The system of claim 2 wherein the sealing element comprises a core that is disposed under a layer that has a surface that is the exterior and both the layer and the core are made of the sealing element material. 5. The system of claim 2 wherein the sealing element material is a polyolefin. 6. The system of claim 2 wherein the sealing element material is a foam. 7. The system of claim 2 wherein the sealing element is hollow. 8. The system of claim 2 wherein the vessel and the port are made from polyethylene and the port threadedly engages the insert such that the insert may be tightened to achieve the seal between the sealing element and the first and second sealing surfaces. 9. A method for holding critical fluids, the method comprising: providing a port on a vessel that is made with polyethylene, has at least about 30 gallons of capacity, and holds a critical fluid that includes a member of the group consisting of sulfuric acid, hydrochloric acid, hydrofluoric acid, tetramethyl ammonium hydroxide, ammonium hydroxide, hydrogen peroxide, phosphoric acid, n-methyl pyridine, isopropyl alcohol, mixtures thereof, and mixtures thereof with other fluids; providing a resilient non-fluoropolymer sealing element comprising a copolymer of ethylene and octene that is corrosion-resistant, essentially impermeable to the contents of the vessel, comprises a material having a Shore A hardness between about 75 and about 95, has less than 1000 ppm total trace metals as measured by digestion in nitric acid and has an exterior that seals against a first sealing surfammonium port and against a second sealing surface on the insert; and mechanically engaging the port and the sealing element with an insert to compress the sealing element to create a seal between the sealing element and the first and second sealing surfaces that is adapted to hold at least 3 psi of air for at least 5 minutes. 10. The method of claim 9 wherein the sealing element material consists essentially of a single material having a Shore A hardness between about 75 and about 90. 11. A system for holding critical fluids, the system comprising: polyethylene holding means for holding at least 30 gallons of fluid; a fluid in the holding means, the fluid being a member of the group consisting of sulfuric acid, hydrochloric acid, hydrofluoric acid, tetramethyl ammonium hydroxide, ammonium hydroxide, hydrogen peroxide, phosphoric acid, n-methyl pyridine, isopropyl alcohol, mixtures thereof, and mixtures thereof with other fluids; a means for fluid egress or ingress of the vessel; an insert means engageable with fluid egress or ingress means; and a non-fluoropolmer means for sealing that cooperates with the insert means and means for fluid egress or ingress of the vessel, the sealing means comprising a copolymer of ethylene and octene and being corrosion-resistant, essentially impermeable to the contents of the vessel, having a Shore A hardness between about 75 and about 95, having less than 1000 ppm total trace metals as measured by digestion in nitric acid, and being adapted to hold at least 3 psi of air for at least 5 minutes.