There are provided processes for extracting aluminum ions from aluminous ores and for preparing alumina. Such processes can be used with various types of aluminous ores such as aluminous ores comprising various types of metals such as Fe, K, Mg, Na, Ca, Mn, Ba, Zn, Li, Sr, V, Ni, Cr, Pb, Cu, Co, Sb,
There are provided processes for extracting aluminum ions from aluminous ores and for preparing alumina. Such processes can be used with various types of aluminous ores such as aluminous ores comprising various types of metals such as Fe, K, Mg, Na, Ca, Mn, Ba, Zn, Li, Sr, V, Ni, Cr, Pb, Cu, Co, Sb, As, B, Sn, Be, Mo, or mixtures thereof.
대표청구항
▼
1. A process for preparing alumina comprising: leaching an aluminous ore with an acid to obtain a leachate and a solid residue, and separating said leachate from said solid residue;removing at least a portion of iron ions contained in said leachate by reacting said leachate with a base to obtain a p
1. A process for preparing alumina comprising: leaching an aluminous ore with an acid to obtain a leachate and a solid residue, and separating said leachate from said solid residue;removing at least a portion of iron ions contained in said leachate by reacting said leachate with a base to obtain a pH of at least 10 and substantially selectively precipitating said at least a portion of iron ions and separating said precipitated at least a portion of iron ions from said leachate to obtain an Al-rich composition;purifying said Al-rich composition; andconverting said purified Al-rich composition into alumina. 2. The process of claim 1, wherein said acid is HCl. 3. The process of claim 2, wherein said aluminous ore is leached with HCl at a temperature of at least 100° C. 4. The process of claim 3, wherein aluminum ions in the form of Al(OH)3 are converted into alumina. 5. The process of claim 1, wherein purifying said Al-rich composition is carried out by precipitating aluminum ions and/or by means of a hollow fiber membrane. 6. The process of claim 5, wherein said pH is at least 11. 7. The process of claim 5, wherein said pH is at least 12. 8. The process of claim 5, wherein said pH is about 11.5 to about 12.5. 9. The process of claim 5, wherein said pH is between 10.5 and 11.0. 10. The process of claim 5, wherein said pH is between 10 and 11. 11. A process for preparing alumina comprising: leaching an aluminous ore with an acid to obtain a leachate and a solid residue, and separating said leachate from said solid residue;at least partially removing iron ions from said leachate by substantially selectively precipitating said iron ions at a pH greater than 10 by reacting said leachate with a base and at least partially removing said precipitated iron ions from said leachate, thereby obtaining an Al-rich composition comprising Al3+ ions;purifying said Al3+ ions; andconverting said Al3+ ions into alumina. 12. The process of claim 11, wherein said acid is HCl. 13. The process of claim 12, wherein said aluminous ore is leached with HCl at a temperature of at least 100° C. 14. The process of claim 13, wherein aluminum ions in the form of Al(OH)3 are converted into alumina. 15. The process of claim 11, wherein purifying said Al3+ ions comprises reacting said Al3+ ions with HCl. 16. The process of claim 11, wherein purifying said Al3+ ions is carried out by selectively precipitating said Al3+ ions and/or by using a hollow fiber membrane. 17. The process of claim 11, wherein purifying said Al3+ ions is carried out by selectively precipitating said Al3+ ions. 18. A process for extracting aluminum ions from an aluminous ore, said process comprising: leaching said aluminous ore with an acid to obtain a composition comprising aluminum ions and iron ions;at least partially removing said iron ions from said composition by substantially selectively precipitating said iron ions at a pH of at least 10 by reacting said composition with a base and at least partially removing said precipitated iron ions, thereby obtaining an Al-rich composition comprising Al3+ ions; andpurifying said Al3+ ions. 19. The process of claim 18, wherein said pH is between 10 and 11. 20. A process for extracting aluminum ions from argillite, said process comprising: leaching said argillite with HCl to obtain a composition comprising a leachate and a solid residue;separating said leachate and said solid residue from one another;at least partially removing iron from said leachate by substantially selectively precipitating iron ions by reacting said leachate with a base and removing a so-formed precipitate, to obtain an Al-rich composition comprising Al3+ ions; andpurifying said Al3+ ions by substantially selectively precipitating said Al3+ ions.