IPC분류정보
국가/구분 |
United States(US) Patent
등록
|
국제특허분류(IPC7판) |
|
출원번호 |
US-0779419
(2010-05-13)
|
등록번호 |
US-8625945
(2014-01-07)
|
발명자
/ 주소 |
- Parris, Don
- Strong, Patrick King
- Matthews, Denise
- Barker, Jeffrey Scott
|
출원인 / 주소 |
|
대리인 / 주소 |
Additon, Higgins, Pendleton & Ashe, P.A.
|
인용정보 |
피인용 횟수 :
3 인용 특허 :
92 |
초록
Disclosed is a low-shrink buffer tube having a reduced diameter. The buffer tube provides adequate crush resistance and is suitable for deployments requiring mid-span access.
대표청구항
▼
1. An optical-fiber buffer tube, comprising: a polymeric tube defining an annular space; anda plurality of optical fibers positioned within the annular space of said polymeric tube, said optical fibers complying with the ITU-T G.652.D recommendations;wherein the annular space of said polymeric tube
1. An optical-fiber buffer tube, comprising: a polymeric tube defining an annular space; anda plurality of optical fibers positioned within the annular space of said polymeric tube, said optical fibers complying with the ITU-T G.652.D recommendations;wherein the annular space of said polymeric tube is substantially free of thixotropic compositions;wherein said optical-fiber buffer tube possesses a buffer-tube filling coefficient that is substantially 0.30 or higher;wherein, upon subjecting said optical-fiber buffer tube to the mid-span testing according to the USDA Rural Electrification Administration mid-span standard, at a wavelength of 1550 nanometers, (i) each of said optical fibers enclosed within said buffer tube has increased attenuation of no more than 0.1 dB and (ii) said optical fibers enclosed within said buffer tube have a mean increased attenuation of no more than 0.05 dB;wherein, upon subjecting said optical-fiber buffer tube to post-extrusion-shrinkage testing in accordance with the TMA method, said buffer tube exhibits post-extrusion shrinkage (PES) of 0.1 percent or less; andwherein said buffer tube has permanent deformations of less than 10 percent after sheave testing. 2. The optical-fiber buffer tube according to claim 1, wherein said optical fibers meet the ITU-T G.657.A1 (11/2009) recommendations and/or the ITU-T G.657.B2 (11/2009) recommendations. 3. The optical-fiber buffer tube according to claim 1, said buffer tube possessing a filling coefficient of at least 0.45. 4. The optical-fiber buffer tube according to claim 1, wherein, upon subjecting said optical-fiber buffer tube to one temperature cycle of the mid-span testing according to the modified USDA Rural Electrification Administration mid-span standard, which includes first measuring attenuation after soaking said optical-fiber buffer tube at 70° C. for 14 hours and thereafter measuring attenuation after soaking said optical-fiber buffer tube at −40° C. for three hours, said optical fibers possess an average change in optical-fiber attenuation of 0.15 dB or less at a wavelength of 1550 nanometers. 5. The optical-fiber buffer tube according to claim 4, wherein, upon subjecting said optical-fiber buffer tube to one temperature cycle of the mid-span testing according to the modified USDA Rural Electrification Administration mid-span standard, at a wavelength of 1550 nanometers, (i) each of said optical fibers enclosed within said buffer tube has increased attenuation of no more than 0.1 dB and (ii) said optical fibers enclosed within said buffer tube have a mean increased attenuation of no more than 0.05 dB. 6. The optical-fiber buffer tube according to claim 1, wherein said buffer tube exhibits excess fiber length (EFL) of no more than 0.25 percent. 7. The optical-fiber buffer tube according to claim 1, wherein said optical fibers, at a wavelength of 1550 nanometers, have a microbending sensitivity of more than 4.0 (dB/km)/(gf/mm) when measured by an expandable drum apparatus at a temperature between −30° C. and 60° C. 8. An optical-fiber buffer tube, comprising: a polymeric tube defining an annular space; anda plurality of optical fibers positioned within the annular space of said polymeric tube, said optical fibers complying with the ITU-T G.657.A1 (11/2009) recommendations and/or the ITU-T G.657.B2 (11/2009) recommendations;wherein the annular space of said polymeric tube is substantially free of thixotropic compositions;wherein said optical-fiber buffer tube possesses a buffer-tube filling coefficient of at least 0.35;wherein, upon subjecting said optical-fiber buffer tube to the mid-span testing according to the USDA Rural Electrification Administration mid-span standard, at a wavelength of 1550 nanometers, said optical fibers enclosed within said buffer tube have a mean increased attenuation of no more than 0.05 dB;wherein, upon subjecting said optical-fiber buffer tube to post-extrusion-shrinkage testing in accordance with the TMA method, said buffer tube exhibits post-extrusion shrinkage (PES) of no more than 0.1 percent; andwherein said buffer tube has permanent deformations of less than 10 percent after sheave testing. 9. The optical-fiber buffer tube according to claim 8, wherein, upon subjecting said optical-fiber buffer tube to the mid-span testing according to the USDA Rural Electrification Administration mid-span standard, each of said optical fibers enclosed within said buffer tube has increased attenuation of no more than 0.1 dB at a wavelength of 1550 nanometers. 10. The optical-fiber buffer tube according to claim 9, wherein said buffer tube exhibits excess fiber length (EFL) of no more than 0.05 percent. 11. The optical-fiber buffer tube according to claim 8, said buffer tube possessing a filling coefficient of at least 0.40. 12. The optical-fiber buffer tube according to claim 11, wherein said buffer tube exhibits excess fiber length (EFL) of no more than 0.25 percent. 13. The optical-fiber buffer tube according to claim 8, said buffer tube possessing a filling coefficient of at least 0.45. 14. The optical-fiber buffer tube according to claim 13, wherein said buffer tube has permanent deformations of less than 5 percent after sheave testing. 15. The optical-fiber buffer tube according to claim 13, wherein said buffer tube exhibits excess fiber length (EFL) of no more than 0.15 percent. 16. The optical-fiber buffer tube according to claim 8, wherein, upon subjecting said optical-fiber buffer tube to one temperature cycle of the mid-span testing according to the modified USDA Rural Electrification Administration mid-span standard, which includes first measuring attenuation after soaking said optical-fiber buffer tube at 70° C. for 14 hours and thereafter measuring attenuation after soaking said optical-fiber buffer tube at −40° C. for three hours, at a wavelength of 1550 nanometers, (i) each of said optical fibers enclosed within said buffer tube has increased attenuation of no more than 0.1 dB and (ii) said optical fibers enclosed within said buffer tube have a mean increased attenuation of no more than 0.05 dB. 17. An optical-fiber buffer tube, comprising: a polymeric tube defining an annular space; anda plurality of optical fibers positioned within the annular space of said polymeric tube, said optical fibers complying with the ITU-T G.657.A1 (11/2009) recommendations and/or the ITU-T G.657.B2 (11/2009) recommendations;wherein the annular space of said polymeric tube is substantially free of thixotropic compositions;wherein said optical-fiber buffer tube possesses a buffer-tube filling coefficient of at least 0.40;wherein, upon subjecting said optical-fiber buffer tube to post-extrusion-shrinkage testing in accordance with the TMA method, said buffer tube exhibits post-extrusion shrinkage (PES) of no more than about 0.1 percent; andwherein, upon subjecting said optical-fiber buffer tube to the mid-span testing according to the USDA Rural Electrification Administration mid-span standard, said optical fibers enclosed within said buffer tube have a mean increased attenuation of no more than 0.05 dB at a wavelength of 1550 nanometers. 18. The optical-fiber buffer tube according to claim 17, wherein, upon subjecting said optical-fiber buffer tube to the mid-span testing according to the USDA Rural Electrification Administration mid-span standard, each of said optical fibers enclosed within said buffer tube has increased attenuation of no more than 0.1 dB at a wavelength of 1550 nanometers. 19. The optical-fiber buffer tube according to claim 18, wherein said buffer tube exhibits excess fiber length (EFL) of no more than 0.15 percent. 20. The optical-fiber buffer tube according to claim 17, wherein, upon subjecting said optical-fiber buffer tube to one temperature cycle of the mid-span testing according to the modified USDA Rural Electrification Administration mid-span standard, which includes first measuring attenuation after soaking said optical-fiber buffer tube at 70° C. for 14 hours and thereafter measuring attenuation after soaking said optical-fiber buffer tube at −40° C. for three hours, at a wavelength of 1550 nanometers, (i) each of said optical fibers enclosed within said buffer tube has increased attenuation of no more than 0.1 dB and (ii) said optical fibers enclosed within said buffer tube have a mean increased attenuation of no more than 0.05 dB. 21. The optical-fiber buffer tube according to claim 17, wherein said buffer tube has permanent deformations of less than 5 percent after sheave testing. 22. The optical-fiber buffer tube according to claim 17, said buffer tube possessing a filling coefficient of at least 0.45. 23. The optical-fiber buffer tube according to claim 22, wherein said buffer tube has permanent deformations of less than 10 percent after sheave testing. 24. The optical-fiber buffer tube according to claim 22, wherein said buffer tube exhibits excess fiber length (EFL) of no more than 0.05 percent. 25. The optical-fiber buffer tube according to claim 22, wherein said polymeric tube comprises nucleated polyethylene, nucleated polypropylene, or a copolymer or a blend thereof. 26. The optical-fiber buffer tube according to claim 17, wherein, upon subjecting said optical-fiber buffer tube to one temperature cycle of the mid-span testing according to the modified USDA Rural Electrification Administration mid-span standard, which includes first measuring attenuation after soaking said optical-fiber buffer tube at 70° C. for 14 hours and thereafter measuring attenuation after soaking said optical-fiber buffer tube at −40° C. for three hours, said optical fibers possess an average change in optical-fiber attenuation of 0.15 dB or less at a wavelength of 1550 nanometers.