초록
▼
In one or more embodiments, a porous composite particulate material includes a plurality of composite particles including an acid-base-resistant core particle at least partially surrounded by one or more layers of acid-base-resistant shell particles. The shell particles are adhered to the core parti
In one or more embodiments, a porous composite particulate material includes a plurality of composite particles including an acid-base-resistant core particle at least partially surrounded by one or more layers of acid-base-resistant shell particles. The shell particles are adhered to the core particle by a polymeric material. The shell particles and/or core particles may be made from an acid-base-resistant material that is stable in harsh chemical conditions. During application of the polymeric material/shell particle bilayer, the core particles are sonicated to homogenize the particle size distribution and minimize agglomeration of particles. Multiple bilayers of polymer/shell particles may be applied. In one embodiment, the core particle comprises generally spherical glassy carbon, while the shell particles may comprise nano-sized diamond particles. Other acid-base-resistant materials may be employed. The porous composite particulate materials may be used in separation technologies, including, but not limited to, chromatography and solid phase extraction.
대표청구항
▼
1. A method for manufacturing a porous composite particulate material, comprising: providing a plurality of acid-base-resistant core particles and a plurality of acid-base-resistant shell particles;applying at least one polymer material/shell particle bilayer comprising: coating at least a portion o
1. A method for manufacturing a porous composite particulate material, comprising: providing a plurality of acid-base-resistant core particles and a plurality of acid-base-resistant shell particles;applying at least one polymer material/shell particle bilayer comprising: coating at least a portion of the plurality of acid-base-resistant core particles, at least a portion of the plurality of acid-base-resistant shell particles, or combinations thereof with polymer material;adhering a portion of the plurality of acid-base-resistant shell particles to each of the plurality of acid-base-resistant core particles with the polymer material to form a plurality of composite particles, wherein at least a portion of the plurality of acid-base-resistant core particles comprises at least one member selected from the group consisting of diamond, graphitic carbon, glassy carbon, silicon carbide, boron nitride, tungsten carbide, niobium carbide, zirconia, noble metals, acid-base-stable highly cross-linked polymers, titania, alumina, and thoria; andapplying sonic energy to the core particles during application of the at least one polymer material/shell particle bilayer to narrow a particle size distribution of the resulting composite particulate material than otherwise would be produced absent application of the sonic energy. 2. The method of claim 1 wherein applying at least one polymer material/shell particle bilayer comprises forming a plurality of polymer material/shell particle bilayers in separate layer-by-layer steps. 3. The method of claim 2 wherein from 5 to 100 of the plurality of polymer material/shell particle bilayers are formed. 4. The method of claim 2 wherein from 10 to 50 of the plurality of polymer material/shell particle bilayers are formed. 5. The method of claim 1 wherein at least a portion of the plurality of acid-base-resistant core particles comprise glassy carbon and the shell particles comprise nano-sized diamond. 6. The method of claim 1 wherein the plurality of composite particles exhibits a particle size of at least about 0.5 μm and a surface area of at least about 5.0 m2/g. 7. The method of claim 1 wherein the plurality of acid-base-resistant core particles exhibits a particle size of at least an order of magnitude larger than the plurality of acid-base-resistant shell particles. 8. The method of claim 1 wherein the polymer material is coated on the core particles before adhering the shell particles to the core particles. 9. The method of claim 1 wherein the polymer material is coated on the acid-base-resistant shell particles before adhering the shell particles to the core particles. 10. The method of claim 1 wherein the sonic energy is applied after coating the polymer material on the core particles and prior to adhering the shell particles of any given bilayer. 11. The method of claim 1 wherein the sonic energy is applied during application of each bilayer. 12. The method of claim 1 wherein the sonic energy is applied during application of any given bilayer in a plurality of discontinuous intervals. 13. The method of claim 11 wherein a total sonication time associated with application of any given bilayer is about 1 minute to about 20 minutes, and wherein each interval is about 5% to about 50% of the total sonication time. 14. The method of claim 11 wherein a total sonication time associated with application of any given bilayer is about 2 minutes to about 10 minutes, and wherein each interval is about 10% to about 30% of the total sonication time. 15. The method of claim 11 wherein a total sonication time associated with application of any given bilayer is about 3 minutes to about 7 minutes, and wherein each interval is about 15% to about 25% of the total sonication time. 16. The method of claim 1, further comprising at least partially cross-linking the polymeric material. 17. A method for manufacturing a porous composite particulate material, comprising: providing a plurality of acid-base-resistant generally spherical core particles and a plurality of acid-base-resistant shell particles;applying at least one polymer material/shell particle bilayer comprising: coating at least a portion of the plurality of acid-base-resistant core particles, at least a portion of the plurality of acid-base-resistant shell particles, or combinations thereof with polymer material;adhering a portion of the plurality of acid-base-resistant shell particles to each of the plurality of acid-base-resistant core particles with the polymer material to form a plurality of composite particles wherein at least a portion of the plurality of acid-base-resistant core particles comprises at least one member selected from the group consisting of diamond, graphitic carbon, glassy carbon, silicon carbide, boron nitride, tungsten carbide, niobium carbide, zirconia, noble metals, acid-base-stable highly cross-linked polymers, titania, alumina, and thoria;at least partially cross-linking the polymeric material; andapplying sonic energy to the core particles during application of the at least one polymer material/shell particle bilayer to reduce a particle size distribution of the resulting composite particulate material than otherwise would be produced absent application of the sonic energy.