최소 단어 이상 선택하여야 합니다.
최대 10 단어까지만 선택 가능합니다.
다음과 같은 기능을 한번의 로그인으로 사용 할 수 있습니다.
NTIS 바로가기AIP advances, v.12 no.6, 2022년, pp.065214 -
Zhu, Fei (College of Materials and Metallurgy, Guizhou University 1 , Guiyang 550000, China) , Liu, Chang (College of Materials and Metallurgy, Guizhou University 1 , Guiyang 550000, China) , Li, Jianlin (College of Materials and Metallurgy, Guizhou University 1 , Guiyang 550000, China) , Zheng, Deyi (College of Materials and Metallurgy, Guizhou University 1 , Guiyang 550000, China) , Pang, Chi (College of Materials and Metallurgy, Guizhou University 1 , Guiyang 550000, China) , Fei, Zihao (Guiyang High-tech YiGe Electronic Co., Ltd. 2 , Guiyang 550000, China)
In this work, the Zn7Sb2O12 spinel phase is pre-synthesized at 980, 1000, 1020, 1040, and 1060 °C by mixing ZnO and Sb2O3 in a molar ratio of 7:1. ZnO varistors are prepared by replacing Sb2O3 with the Zn7Sb2O12 spinel phase. The effect of the Zn7Sb2O12 spinel on the electrical properties and mi...
Jpn. J. Appl. Phys. 10 736 1971 10.1143/jjap.10.736 Nonohmic properties of zinc oxide ceramics
Ceram. Int. 45 11105 2019 10.1016/j.ceramint.2019.01.260 Stable electrical properties of ZnO varistor ceramics with multiple additives against the AC accelerated aging process
AIP. Adv. 6 030701 2016 10.1063/1.4944485 Electrical degradation of double-Schottky barrier in ZnO varistors
J. Phys.: Condens. Matter 26 115801 2014 10.1088/0953-8984/26/11/115801 Electron paramagnetic resonance study of ZnO varistor material
Jpn. J. Appl. Phys. 42 1 2003 10.1143/jjap.42.1 Base-metal electrode-multilayer ceramic capacitors: Past, present and future perspectives
J. Mater. Res. 30 2300 2015 10.1557/jmr.2015.199 Nonlinear property of SrCoO3-doped ZnO ceramics sintered in a reducing atmosphere and multilayer ceramic varistors with base metal electrodes
J. Alloys Compd. 834 155070 2020 10.1016/j.jallcom.2020.155070 Influence of Bi3Zn2Sb3O14 pre-synthesis phase on electrical properties of the ZnO-Bi2O3 based varistor ceramics
J. Electroceram. 18 175 2007 10.1007/s10832-007-9023-8 Microstructural and electrical properties of multicomponent varistor ceramics with PbO-ZnO-B2O3 glass addition
Int. J. Appl. Ceram. Technol. 9 960 2012 10.1111/j.1744-7402.2011.02702.x Two-step sintering of pristine and aluminum-doped zinc oxide ceramics
Ceram. Int. 46 14913 2020 10.1016/j.ceramint.2020.03.018 Flash sintering preparation and electrical properties of ZnO-Bi2O3-M (M = Cr2O3, MnO2 or Co2O3) varistor ceramics
Ceram. Int. 38 S457 2012 10.1016/j.ceramint.2011.05.039 Electrical properties of Al2O3-doped ZnO varistors prepared by sol-gel process for device miniaturization
J. Eur. Ceram. Soc. 27 1101 2007 10.1016/j.jeurceramsoc.2006.05.040 ZnO varistors with reduced amount of additives prepared by direct mixing of constituent phases
J. Am. Ceram. Soc. 94 3871 2011 10.1111/j.1551-2916.2011.04575.x Comparative study of microstructure and electrical properties of varistors prepared from plasma vapor-phase reaction process and French process ZnO powders
Ceram. Int. 42 10547 2016 10.1016/j.ceramint.2016.03.042 Influence of Cr2O3 on highly nonlinear properties and low leakage current of ZnO-Bi2O3 varistor ceramics
Mater. Chem. Phys. 63 157 2000 10.1016/s0254-0584(99)00227-8 Electrical properties of varistors in relation to their true bismuth composition after sintering
J. Mater. Sci. 24 213 1989 10.1007/bf00660956 Sintering of Sb2O3-doped ZnO
J. Mater. Sci. 22 2229 1987 10.1007/bf01132965 Studies on microstructure and density of sintered ZnO-based non-linear resistors
J. Am. Ceram. Soc. 73 1817 1990 10.1111/j.1151-2916.1990.tb05232.x Application of zinc oxide varistors
Ceram. Int. 47 4118 2021 10.1016/j.ceramint.2020.09.288 Low temperature sintering ZnO-Bi2O3 based varistor ceramics with low electrical breakdown voltage and high nonlinear coefficient
Beilstein J. Nanotechnol. 12 49 2021 10.3762/bjnano.12.4 ZnO and MXenes as electrode materials for supercapacitor devices
Nanoscale 13 9160 2021 10.1039/d1nr00943e About defect phenomenon in ZnO nanocrystals
Nanoscale 12 12790 2020 10.1039/d0nr02028a Synergy of nano-ZnO and 3D-graphene foam electrodes for asymmetric supercapacitor devices
J. Am. Ceram. Soc. 98 1356 2015 10.1111/jace.13453 Influence of WO3-doping on the microstructure and electrical properties of ZnO-Bi2O3 varistor ceramics sintered at 950 °C
J. Am. Ceram. Soc. 100 3024 2017 10.1111/jace.14863 Preparation and electrical properties of ZnO-Bi2O3-based multilayer varistors with base metal nickel inner electrodes
J. Eur. Ceram. Soc. 35 3535 2015 10.1016/j.jeurceramsoc.2015.05.035 High performance varistors prepared from doped ZnO nanopowders made by pilot-scale flame spray pyrolyzer: Sintering, microstructure and properties
Appl. Phys. Lett. 79 48 2001 10.1063/1.1378051 Role of oxygen at the grain boundary of metal oxide varistors: A potential barrier formation mechanism
※ AI-Helper는 부적절한 답변을 할 수 있습니다.