NTIS 바로가기Fibre chemistry, v.35 no.4, 2003년, pp.265 - 269
Perepelkin, K. E. (St. Petersburg State University of Technology and Design) , Andreeva, I. V. (St. Petersburg State University of Technology and Design) , Pakshver, E. A. (All-Russian Scientific-Research Institute of Synthetic Fibres, Tver') , Morgoeva, I. Yu. (St. Petersburg State University of Technology and Design)
Comparative studies of the thermal characteristics of para-aramid fibres (Armos, Rusar, Terlon, Twaron, and Kevlar) were conducted using thermomechanical analysis (TMA), dynamic thermogravimetric analysis (TGA), and differential scanning calorimetry (DSC). According to the TMA data, the para-aramid fibres studied are characterized by dimensional stability up to temperatures of 400-450°C; shrinkage or spontaneous elongation does not exceed 0.5-1%. TGA and DSC revealed the temperature characteristics of the para-aramid fibres corresponding to the occurrence of thermooxidative degradation. These processes begin at 400-450°C and are accompanied by shrinkage; 4% weight loss takes place at temperatures above 490-500°C.
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.