NTIS 바로가기Vacuum, v.82 no.2, 2007년, pp.252 - 256
Cekada, M. (Jozef Stefan Institute, Jamova 39, 1000 Ljubljana, Slovenia) , Panjan, P. , Kek-Merl, D. , Panjan, M. , Kapun, G.
Hard coating defects are produced by foreign particle contamination on substrate surface before and during coating, or due to arcing. In this work, CrN, TiAlN and CrN/TiAlN multilayer hard coatings were prepared by thermoionic arc ion plating deposition system BAI 730 (Balzers) and by sputter deposi...
Vacuum Munz 46 323 1995 10.1016/0042-207X(94)E0029-X
Surf Coat Technol Mitterer 89 233 1997 10.1016/S0257-8972(96)02908-8
Wear Wiklund 232 262 1999 10.1016/S0043-1648(99)00155-6
Surf Coat Technol Wang 126 279 2000 10.1016/S0257-8972(00)00554-5
Surf Coat Technol Jehn 125 212 2000 10.1016/S0257-8972(99)00551-4
Thin Solid Films Lewis 503 143 2006 10.1016/j.tsf.2005.08.375
Surf Coat Technol Koski 115 163 1999 10.1016/S0257-8972(99)00172-3
J Vac Technol A Helmersson 3 308 1985 10.1116/1.573256
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.