조민우 (경희대학교 대학원 치의학과 치과보존학교실) , 박상혁 (경희대학교 대학원 치의학과 치과보존학교실) , 김종률 (경희대학교 대학원 치의학과 치과보존학교실) , 최경규 (경희대학교 대학원 치의학과 치과보존학교실)
The objectives of this study was to evaluate the durability of 4 resin cements by means of microtensile bond strength test combined with thermocycling method and fractographic FE-SEM analysis. Experimental groups were prepared according to thermocycling (0, 1,000, 5,000) and the kind of resin cement...
Manhart J, Scheibenhogen Fuchsbrunner A, Chen HY, Hiekel R. A 2-year clinical study of composite and ceramic inlays. Olin Oral Invest 4: 192-8, 2000
Peumans M, Van Meerbeek B, Lambrechts P, Vanherle G. Porcelain Veneers: a review of the literature. J Dent 28:163-77, 2000
Mitchell CA, Abbariki M, Orr JF. The influence of luting cement on the probabilities of survival and modes of failure of cast full-coveraged crowns. Dent Mater 16:198-206, 2000
Knox J, Kralj B, Hubsch PF, Middleton J, Jones ML. An evaluation of the influence of orthodontic adhesive on the stresses generated in a bonded bracket finite element model. Am J Ortho Dent Orthop 119:43-53, 2001
el-Mowafy O, Rubo MH. Retention of a posterior resinbonded fixed partial denture with a modified design : an in vitro study. Int J Prosthod 13:425-31. 2000
Carvalho RM, Pegoraro TA, Tay FR. Pegoraro LF, Pashley DH. Adhesive permeability affects coupling of resin cements that utiliseself-etching primers to dentine. J Dent 32:55-65, 2004
Kramer N, Lohbauer D, Frankenberger R. Adhesive luting of indirect restorations. Am J Dent 13:60D-76D, 2000
Hasegawa EA, Boyer DB, Chan DC. Hardening of dual-cured cements under composite resin inlays. J Prosthet Dent 66:187-92, 1991
el-Badrawy WA, el-Mowafy OM. Chemical versus dual curing of resin inlay cements, J Prosththet Dent 73:515-24, 1995
Primenta LAF, Amaral CM, Bredrane de Castro AKB, Ritter AV. Stability of dentin bond strengths using different bonding techniques after Total-etch, deproteinization and self-etching. Oper Dent 29:592-598
Paul SJ, Welter DA, Ghazi M, Pashley D. Nanoleakage at the dentin adhesivevs. microtensile bond strength. Oper Dent 24:181-188, 1999
Giannini M, Seixas CAM, Reis AF, Pimenta LAF. Six-month storage-time evaluation of one-bottle adhesive systems to dentin. J Esth Rest Dent 15:43-49, 2003
Tay FR. Pashley DH, Yoshiyama M. Two mondes of nanoleakage expression in single-step adhesives. J Dent Res 81 :472-476, 2002
Sano H. Yoshikawa T, Pereira PNR, Kanemura N, Morigami M, Tagami J, Pashley D. Long-term Durability of dentine bonds made with a self-etching primer. J Dent Res 78:906-911, 1999
Kato G, Nakabayashi N. The durability of adhesion to phosphoric acid etched, wet dentine substrates. Dent Mater 14:347-352, 1998
Hakimeh S, Vaidyanathan J, Houpt ML, Vaidyanathan TK, Hagen SV. Microleakage of compomer class V restorations: effect of load cycling, thermal cycling, and cavity shape differences. J Prosthet Dent 83: 194-203, 2000
Wendt SL, Mcinnes PM, Dickinson GL. The effect of thermocycling in microleakage analysis. Dent Mater 8: 181-184, 1992
Miyazaki M, Sato M, Onose H. Moore BK. Influence of thermal cycling on dentin bond strength of two-step bonding systems. Am J Dent 11: 118- 122, 1998
Hashimoto M, Ohno H. Kaga M, Endo K, Sano H. Oguchi H. In vivo degradation of resin-dentin bonds in humans over 1 to 3 years. J Dent Res 79:1385-1391. 2000
Krejci I, Lutz F. Mixed class V restorations: the potentials of dentine bonding. J Dent 18:263-270, 1990
Suh BI, Feng L, Pashley DH. Tay FR. Factors contributing to the incompatibility between simplified-step adhesives and chemically-cured or dual-cured composites. Part III. Effect of acidic resin monomers. J Adhes Dent 5:267-282, 2003
Attal JP, Asmussen E, Degrange M. Effects of surface treatment on the free surface energy of dentin. Dent Mater 10:259-264, 1994
Tay FR. Pashley DH. Aggressiveness of contemporary self-etching systems. I: Depth of penetration beyond dentin smear layers. Dent Mater 17:296-308, 2001
Frankenberger R, Strobel WO, Lohbauer U, Kramer N, Petschelt A. The effect of six years of water storage on resin composite bonding to human dentin. J Biomed Mater Res Part B: Appl Biomater 69:25-32, 2004
Armstrong SR, Vargas MA, Fang Q, Laffoon JE. Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1-step dentin bonding system through 15-month water storage. J Adhes Dent 5:47-56, 2003
Tay FR. Pashley DH. Dental adhesives of the future. J Adhes Dent 4:91-103, 2002
Brackett MG, Dib A. Brackett WW, Estrada BE, Reyes AA. One-year clinical performance of a resin-modified glass ionomer and a resin composite restorative material in unprepared Class V restorations. Oper Dent 27: 112-6, 2002
Turkun SL. Clinical evaluation of a self-etching and a one-bottle adhesive system at two years. J Dent 31: 527-534, 2003
Takahashi A, Inoue S, Kawamoto C, Ominato R, Tanaka T, Sato Y, Pereira PNR. Sano H. In vivo long-term durability of the bond to dentin using two adhesive systems. J Adhes Dent 4:151-159, 2002
Miyazaki M, Sato M, Onose H. Moore BK. Influence of thermal cycling on dentin bond strength of two-step bonding systems. Am J Dent 11: 118-122, 1998
Nikaido T, Kunzelman KH. Chen H, Ogata M, Harada N, Yamaguchi S, Cox CF, Hickel R, Tagami J. Evaluation of thermal cycling and mechanical loading on bond strength of a self-etching primer system to dentin. Dent Mater 18:269-275, 2002
Jan DM, Marcos V, Kirsten VL, Kazuhiro H. Paul L, Bart VM. Bonding of an auto-adhesive luting material to enamel and dentin. Dent Mater 20:963-971. 2004
Bin Y, Klaus L, Rainer A. Matthias K. Microtensile bond strength of three luting resins to human regional dentin. Dent Mater 22:45-46, 2006
※ AI-Helper는 부적절한 답변을 할 수 있습니다.