NTIS 바로가기Journal of the Korean Recycled Construction Resources Institute = 한국건설순환자원학회 논문집, v.9 no.2, 2021년, pp.177 - 184
구경모 (한화건설 건축사업본부 기술혁신팀) , 최재원 (아세아시멘트 기술연구소) , 유병노 (아세아시멘트 기술연구소) , 차완호 (아세아시멘트 기술연구소) , 강봉희 (아세아시멘트)
In this study, the effects of ground granulated blast furnace slag(GGBFS) and expansive additive(EA) on early strength mortar were examined for the purpose of reducing carbon and improving cement performance. As a result, ealry strength Portland cement(EPC) tended to decrease in flow compared to ord...
Hester, D., Mcnally, C., Richardson, M.G. (2005). Study of influence of slag alkali level on the alkali-silica reactivity of slag concrete, Construdction and Building Materials, 19(9), 661-665.
Hosan, A., Shaikh, F.U.A. (2021). Compressive strength development and durability properties of high volume slag and slag-fly ash blended concretes containing nano-CaCO 3 , Journal of Materials Research and Technology, 6, 1310-1322.
Japan Cement Association. (1993). Easy to Understand for Cement Science, Japan: Japan Cement Association.
Jeong, I.D., Lee, T.W., Koo, K.M., Jang, S.S., Jung, Y.W., Kwon, Y.H. (2018). Compressive strength and deformation of high strength mortar with CaO-gypsum, The Proceedings of the Korea Concrete Instetute, 30(1), 163-164.
Kim, K., Choi, H., Yoon, S., Kim, J., Gong, M., Jeong, Y. (2017). An experimental study on the reduction of construction period in the winter season using high early strength cement, Proceeding of Korea Concrete Institute, 473~474.
Koh, K.T., Cheong, H.M. (2005). Properties of concrete to curing temperature, Korea Concrete Institute, 17(1), 22-27.
Lee, E.B., Ko, J.W., Yoo, J.K., Kim, G.T., Song, D.G., Koo, K.M. (2020). Early age strength of concrete using high fineness ordinary portland cement and powdered early strength admixture, 36(7), 163-171.
Lee, S.H., Lee, K.H., Yoo, D.W., Ha, J.H., Cho, Y.G. (2015). Hydration and insulation characteristics of a ground granulated blast furnace slag based non-sintered cement using circulating fluidzed bed combustion ash as a activator, Journal of the Korea Concrete Institute, 27(3), 245-252.
Lee, T.G., Kim, Y.R., Song, Y.C., Lee, J.H., Park, C.J. Park, J.H. (2019). Evaluation on strength development of high early strength concrete for horizontal form removal, Proceeding of Korea Concrete Institute, 517-518.
Leng, F., Feng, N., Lu, X. (2000). An experiment study on the properties of resistance to diffusion of chloride ions of fly ash and blast furnace slag concrete, Cement and Concrete research, 30, 989-992.
Lim, S.N., Wee, T.H. (2020). Autogenous shrinkage of ground -granulated blast furnace slag concrete, ACI Materials Journal, 97(5), 587-593.
Park, C.Y., Kang, B.H. (2008). A study on rheological properties of cement paste using expansive additives by kind & replacement ratio, Journal of the Korea Institute of Building Construction, 8(2), 99-106.
Ryu, D.W., Kim, W.J., Yang, W.H., You, J.H., Ko, J.W. (2012). An experimental study on the freezing-thawing and chloride resistance of concrete using high volumes of GGBFS, Journal of the Korea Institute of Building Construction, 12(3), 315-322.
Siddique, R., Bennacer, R. (2012). Use of iron and steel industry by-product (GGBS) in cement paste and mortar, Resources Conservation and Recycling, 69, 29-34.
Yang, K.H., Cho, A.R., Song, J.K., Nam, S.H. (2012). Hydration products and strength development of calcium hydroxide-based alkali-activated slag mortars, Construction and Building Materials, 29, 410-419
Zhang, H.Y., Kiu, J.C., Wu, B. (2021). Mechanical properties and reaction mechanism of one-part geopolymer mortars, Construction and Building Materials, 273(2), 121973.
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
오픈액세스 학술지에 출판된 논문
※ AI-Helper는 부적절한 답변을 할 수 있습니다.