NTIS 바로가기Journal of alloys and compounds, v.694, 2017년, pp.1073 - 1082
Ponnilavan, V. , Kannan, S.
The crystallization, morphological and mechanical behavior of excess ceria additions in zirconia toughened alumina (ZTA) systems is investigated. The results reveal the crucial role of ceria in the thermal stability of ZTA systems. The pure ZTA system indicated degraded to yield monoclinic zirconia ...
Biomaterials De Aza 23 937 2002 10.1016/S0142-9612(01)00206-X Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses
J. Mater. Res. Ebrahimi 15 142 2000 10.1557/JMR.2000.0024 Slow crack growth behavior of alumina ceramics
J. Bone Jt. Surg. Am. Clarke 85 73 2003 10.2106/00004623-200300004-00009 Current status of zirconia used in total hip implants
J. Am. Ceram. Soc. Pezzotti 91 1199 2008 10.1111/j.1551-2916.2007.01507.x Raman spectroscopic analysis of advanced ceramic composite for hip prosthesis
Biomaterials Chevalier 30 5279 2001 10.1016/j.biomaterials.2009.06.022 On the kinetics and impact of tetragonal to monoclinic transformation in an alumina/zirconia composite for arthroplasty applications
Dent. Mater. Fabbria 30 138 2014 10.1016/j.dental.2013.10.006 Lifetime estimation of a zirconia-alumina composite for biomedical applications
J. Eur. Ceram. Soc. Deville 23 2975 2003 10.1016/S0955-2219(03)00313-3
Acta Biomater. Kohorst 8 1213 2012 10.1016/j.actbio.2011.11.016 Low-temperature degradation of different zirconia ceramics for dental applications
Mater. Chem. Phys. Pandey 146 456 2014 10.1016/j.matchemphys.2014.03.053 In vitro ageing and wear behaviour of ceria stabilized zirconia toughened alumina (CSZ-TA) bio-ceramic
Mater. Sci. Eng. A Rejab 595 18 2014 10.1016/j.msea.2013.11.091 Effects of MgO addition on the phase, mechanical properties, and microstructure of zirconia-toughened alumina added with CeO2 (ZTA-CeO2) ceramic composite
J Prosthodont. Res. Tanaka 59 55 2015 10.1016/j.jpor.2014.11.006 A 3-year follow-up of ceria-stabilized zirconia/alumina nanocomposite (Ce-TZP/A) frameworks for fixed dental prostheses
Biomaterials Benzaid 29 3636 2008 10.1016/j.biomaterials.2008.05.021 Fracture toughness, strength and slow crack growth in a ceria stabilized zirconia-alumina nanocomposite for medical applications
Biomaterials Studart 28 2695 2007 10.1016/j.biomaterials.2006.12.033 In vitro lifetime of dental ceramics under cyclic loading in water
J. Eur. Ceram. Soc. de Bernardi-Martin 34 4469 2014 10.1016/j.jeurceramsoc.2014.06.024 Grain-boundary cation diffusion in ceria tetragonal zirconia determined by constant-strain-rate deformation tests
Chem. Mater. Hao 26 6073 2014 10.1021/cm503131p Ceria?Zirconia solid solutions (Ce1?xZrxO2?δ, x ≤ 0.2) for solar thermochemical water splitting: a thermodynamic study
Acta Mater. Kuhn 61 4277 2013 10.1016/j.actamat.2013.04.001 Structural characterization and oxygen nonstoichiometry of ceria-zirconia (Ce1-xZrxO2?δ) solid solutions
Cryst. Struct. Wyckoff 1 7 1963
Acta Cryst. Sect. B Howard 44 116 1988 10.1107/S0108768187010279 Structures of the ZrO2 polymorphs at room temperature by high-resolution neutron powder diffraction
Z. fur Kristallogr. Newnham 117 235 1962 10.1524/zkri.1962.117.2-3.235 Refinement of the α-Al2O3, Ti2O3, V2O3 and Cr2O3structures
J. Am. Ceram. Soc. Zhang 89 1028 2006 10.1111/j.1551-2916.2005.00788.x Phases in ceria-zirconia binary oxide (1-x)CeO2-xZrO2 nanoparticles: the effect of particle size
Catal. Lett. Reddy 130 227 2009 10.1007/s10562-009-9870-9 Microwave-assisted synthesis and structural characterization of nanosized Ce0.5Zr0.5O2 for CO oxidation
J. Am. Ceram. Soc. Vasanthavel 97 3774 2014 10.1111/jace.13182 Phase Stabilization of ZrO2 Polymorph by combined additions of Ca2+ and PO43- ions through an in situ synthetic approach
Philos. Mag. Sharma 84 2731 2004 10.1080/14786430410001671467 Observation of dynamic nanostructural and nanochemical changes in ceria-based catalysts duringin-situ reduction
Ultramicroscopy Crozier 108 1432 2008 10.1016/j.ultramic.2008.05.015 In situ environmental TEM studies of dynamic changes in cerium-based oxides nanoparticles during redox processes
Acta Biomater. Flamant 2016 10.1016/j.actbio.2016.09.017 Selective etching of injection molded zirconia-toughened alumina: towards osseointegrated and antibacterial ceramic implants
Mater. Sci. Eng. A Pulgarin 639 136 2015 10.1016/j.msea.2015.05.010 Three different alumina-zirconia composites: sintering, microstructure and mechanical properties
J. Power Sources Gao 195 3130 2010 10.1016/j.jpowsour.2009.11.117 Effect of zinc oxide on yttria doped ceria
Ind. Eng. Chem. Res. Rao 50 11960 2011 10.1021/ie201474p Structural characterization and catalytic evaluation of supported copper a ceria catalysts for soot oxidation
Solid State Sci. Escribano 5 1369 2003 10.1016/j.solidstatesciences.2003.07.001 Characterization of cubic ceria-zirconia powders by X-ray diffraction and vibrational and electronic spectroscopy
Appl. Catal. A Bensalem 121 81 1995 10.1016/0926-860X(95)85012-0 Preparation and characterisation of highly dispersed silica supported ceria
Phys. Rev. B Sundaresan 74 161306R 2006 10.1103/PhysRevB.74.161306 Ferromagnetism as a universal feature of nanoparticles of the otherwise nonmagnetic oxides
J. Appl. Phys. McBride 76 2435 1994 10.1063/1.357593 Raman and X-ray studies of Ce1-xRExO2-y, where RE=La, Pr, Nd, Eu, Gd, and Tb
Science Esch 309 752 2005 10.1126/science.1111568 Electron localization determines defect formation on ceria substrates
Nanoscale Res. Lett. Phokha 7 425 2012 10.1186/1556-276X-7-425 Synthesis, characterization, and magnetic properties of monodisperse CeO2 nanospheres prepared by PVP-assisted hydrothermal method
J. Am. Ceram. Soc. Claussen 59 49 1976 10.1111/j.1151-2916.1976.tb09386.x Fracture toughness of Al2O3 with an unstabilized ZrO2 dispersed phase
J. Mater. Sci. Wang 24 3421 1989 10.1007/BF02385721 Zirconia-toughened alumina (ZTA) ceramics
Biomaterials Affatato 20 1925 1999 10.1016/S0142-9612(99)00093-9 Mixed oxides prosthetic ceramic ball heads. Part 2: effect of the ZrO2 fraction on the wear of ceramic on ceramic joints
*원문 PDF 파일 및 링크정보가 존재하지 않을 경우 KISTI DDS 시스템에서 제공하는 원문복사서비스를 사용할 수 있습니다.
※ AI-Helper는 부적절한 답변을 할 수 있습니다.