NTIS 바로가기전기화학회지 = Journal of the Korean Electrochemical Society, v.27 no.1, 2024년, pp.40 - 46
김민진 (한국공학대학교 융합기술에너지대학원) , 류지헌 (한국공학대학교 융합기술에너지대학원)
Among the electrode manufacturing processes for lithium-ion batteries, the drying process is crucial for production speed and process cost. Particularly, as the loading level of the electrode increases to enhance the energy density of the battery, optimizing process conditions for electrode drying b...
T.-H. Kim, J.-S. Park, S. K. Chang, S. Choi, J. H. Ryu,?and H.-K. Song, The current move of lithium ion?batteries towards the next phase, Adv. Energy Mater.,?2(7), 860 (2012).
H. Li, Z. X. Wang, L. Q. Chen, and X. J. Huang,?Research on advanced materials for Li-ion batteries, Adv.?Mater., 21(45), 4593 (2009).
S. Megahed and B. Scrosati, Lithium-ion rechargeable?batteries, J. Power Sources, 51(1-2), 79 (1994).
Y. Kuang, C. Chen, D. Kirsch, and L. Hu, Thick?electrode batteries: Principles, opportunities, and?challenges, Adv. Energy Mater., 9(33), 1901457 (2019).
M. Singh, J. Kaiser, and H. Hahn, Thick electrodes for?high energy lithium ion batteries, J. Electrochem. Soc., 162, A1196 (2015).
H. Kim and J. H. Ryu, Effect of electrode design on?electrochemical performance of highly loaded LiCoO 2 ?positive electrode in lithium-ion batteries, J. Korean?Electrochem. Soc., 23(2), 47 (2020).
J. M. Kang, H. W. Kim, Y. S. Jang, H. Kim, and J. H.?Ryu, Thick positive electrode using?polytetrafluorethylene (PTFE) binder for high-energy-density lithium-ion batteries, J. Korean Electrochem.?Soc., 24(2), 28 (2021).
R. Sahore, D. L. Wood III, A. Kukay, K. M. Grady, J. Li,?and I. Belharouak, Towards understanding of cracking?during drying of thick aqueous-processed?LiNi 0.8 Mn 0.1 Co 0.1 O 2 cathodes, ACS Sustainable Chem.?Eng., 8(8), 3162 (2020).
J. Kumberg, M. Muller, R. Diehm, S. Spiegel, C.?Wachsmann, W. Bauer, P. Scharfer, and W. Schabel,?Drying of lithium-ion battery anodes for use in high-energy cells: Influence of electrode thickness on drying?time, adhesion, and crack formation, J. Energy Technol.,?7(11), 1900722 (2019).
S. Ahmed, P. A. Nelson, K. G. Gallagher, and D. W.?Dees, Energy impact of cathode drying and solvent?recovery during lithium-ion battery manufacturing, J.?Power Sources, 322, 169 (2016).
M. Ryu, Y.-K. Hong, S.-Y. Lee, and J. H. Park, Ultrahigh?loading dry-process for solvent-free lithium-ion battery?electrode fabrication, Nat. Commun., 14, 1316 (2023).
Y. S. Zhang, J. J. Bailey, Y. Sun, A. M. Boyce, W.?Dawson, C. D. Reynolds, Z. Zhang, X. Lu, P. Grant, E.?Kendrick, P. R. Shearing, and D. J. L. Brett, Applications?of advanced metrology for understanding the effects of?drying temperature in the lithium-ion battery electrode?manufacturing process, J. Mater. Chem. A, 10(19), 10593?(2022).
M. Muller, L. Pfaffmann, S. Jaiser, M. Baunach, V.?Trouillet, F. Scheiba, P. Scharfer, W. Schabel, and W.?Bauer, Investigation of binder distribution in graphite?anodes for lithium-ion batteries, J. Power Source, 340, 1?(2017).
B. G. Westphal and A. Kwade, Critical electrode?properties and drying conditions causing component?segregation in graphitic anodes for lithium-ion batteries,?J. Energy Storage, 18, 509 (2018).
B. Westphal, H. Bockholt, T. Gunther, W. Haselrieder,?and A. Kwade, Influence of convective drying?parameters on electrode performance and physical?electrode properties, ECS Trans., 64, 57 (2015).
S. S. Hwang, M. Sohn, H.-I. Park, J.-M. Choi, C.G. Cho,?and H. Kim, Effect of the heat treatment on the?dimensional stability of Si electrodes with PVDF binder,?Electrochim. Acta, 211, 356 (2016).